Parker Lord

Parker LORD

Parker LORD Structural Adhesives, Thermal Management & Electronic Materials

Parker LORD develops engineered materials for structural bonding, thermal management, semiconductor and electronic assembly, surface preparation, and elastomer bonding. The portfolio includes LORD epoxy, structural acrylic, urethane, and specialty adhesive systems; COOLTHERM materials for thermal management and electronic packaging; and Chemlok materials for rubber-to-substrate bonding.

As an authorized Parker LORD distributor, Krayden supplies a selection of structural adhesives, COOLTHERM thermal-management and electronic materials, Chemlok bonding systems, and related surface-preparation products. Our team can help customers compare adhesive chemistry, substrates, bond or gap geometry, thermal requirements, dispensing methods, cure processes, electrical requirements, and other application-specific considerations.

Markets Served by Parker LORD

Aerospace & Defense Automotive & Transportation Electric Vehicles & Electrification Electronics & Semiconductors Industrial Manufacturing Energy Marine

Featured Parker LORD Brands

Key Parker LORD brands supporting structural bonding, thermal management, electronic packaging, and rubber-to-substrate bonding.

LORD brand logo placeholder

LORD

Structural adhesive systems spanning epoxy, structural acrylic, urethane, and specialty chemistries for engineered assembly. Product selection depends on substrates, bond geometry, cure and handling requirements, and the mechanical demands of the finished assembly.

COOLTHERM brand logo placeholder

COOLTHERM

Thermal-management and electronic materials including thermally conductive adhesives, gap fillers, gels, potting and encapsulation systems, die-attach materials, and semiconductor-package protection products.

Chemlok brand logo placeholder

Chemlok

Elastomer-bonding materials for rubber-to-metal and rubber-to-substrate applications, including systems used during molding and specialized bonding processes.

 
Parker LORD structural adhesive application
LORD Structural Bonding Systems

Structural Adhesives

Parker LORD structural adhesives include epoxy, structural acrylic, urethane, and specialty systems for joining metals, composites, plastics, and other engineered assemblies. Different chemistries address different combinations of cure speed, stiffness or flexibility, gap filling, impact and peel requirements, substrate preparation, and production method.

LORD epoxy structural adhesive image placeholder
Chemistry

Epoxy Adhesives

Two-component epoxy systems provide structural bonding options for metal, composite, plastic, and other engineered assemblies where controlled cure and durable attachment are required.

LORD structural acrylic adhesive
Chemistry

Structural Acrylic Adhesives

Structural acrylic adhesives support fast production bonding of metals, plastics, composites, and mixed-material assemblies where rapid handling, impact and peel performance, gap filling, or reduced surface preparation are important.

LORD 7550 urethane adhesive
Chemistry

Urethane & Specialty Adhesives

Urethane and specialty adhesive systems provide alternatives for assemblies that benefit from flexibility, stress distribution, or bonding of engineered composites and plastics.

 
Parker LORD thermal management application
COOLTHERM Thermal Management Materials

Thermal Management Materials

COOLTHERM materials support thermal interfaces and component protection in EV batteries, power electronics, motors, semiconductor assemblies, and other heat-generating systems. The portfolio includes thermally conductive adhesives, dispensable gap fillers, gels, and potting or encapsulation systems.

COOLTHERM thermally conductive adhesive image placeholder
Thermal Function

Thermally Conductive Adhesives

Bonding materials that provide structural attachment while creating a conductive thermal pathway between heat-generating components and cooling structures.

COOLTHERM SC-1600 gap filler image placeholder
Interface Format

Gap Fillers

Dispensable gap fillers conform to dimensional variation between heat-generating components and cooling surfaces to maintain a continuous thermal interface.

COOLTHERM thermal gel image placeholder
Dispensable Thermal Interface

Thermally Conductive Gels

Thermally conductive gels provide a compliant dispensable interface for assemblies where low mechanical stress, dimensional variation, and thermal transfer are important.

COOLTHERM potting and encapsulation image placeholder
Protection Method

Potting & Encapsulation

Potting and encapsulation materials protect electrical and electronic components while supporting thermal, dielectric, environmental, and mechanical requirements.

 
Chemlok rubber-to-substrate bonding application image placeholder
Chemlok Elastomer Bonding Systems

Rubber-to-Substrate Bonding

Chemlok bonding systems are used to bond rubber and other elastomers to metal and selected rigid substrates during molding, curing, and specialized post-vulcanization processes. Product selection depends on elastomer type, substrate, molding conditions, cure temperature, surface preparation, and required environmental resistance.

Chemlok rubber bonding material image placeholder
Elastomer Bonding

Rubber-to-Metal & In-Mold Bonding

Chemlok products support molded rubber components where reliable adhesion to prepared metal or other rigid substrates must withstand mechanical, thermal, and environmental service conditions.

Chemlok primer and specialty elastomer bonding image placeholder
Bond Preparation & Specialty Systems

Primers & Specialty Elastomer Bonding

Chemlok primers and specialized one-coat or multi-step systems extend elastomer bonding across different rubber compounds, urethanes, substrate combinations, and manufacturing processes.

 
Parker LORD semiconductor packaging application image placeholder
COOLTHERM Microelectronic Materials

Electronic Assembly & Semiconductor Packaging

Parker LORD electronic materials support semiconductor die attachment, package underfill, encapsulation, and related electronic assembly requirements. Selection depends on package architecture, thermal and electrical requirements, cure conditions, flow behavior, coefficient-of-thermal-expansion considerations, reliability targets, and manufacturing process.

COOLTHERM die attach adhesive image placeholder
Semiconductor Assembly

Die Attach & Conductive Adhesives

Die-attach materials bond semiconductor devices to package structures while supporting thermal and mechanical requirements in processors, power devices, and other microelectronic assemblies.

COOLTHERM underfill material image placeholder
Package Protection

Underfills & Package Encapsulants

Underfill materials flow beneath semiconductor packages to reinforce solder interconnects and help manage mechanical stresses generated by thermal cycling, shock, vibration, and differences in thermal expansion.

 
Parker LORD surface preparation application image placeholder
LORD Bond Preparation Materials

Surface Preparation Materials

Parker LORD surface-preparation materials include primers, accelerators, and adhesion promoters used with selected adhesive and elastomer-bonding processes. These products should be matched to the exact adhesive system, substrate condition, cleaning method, and production sequence.

Primers

Primers condition properly prepared substrates before selected adhesive or elastomer-bonding processes. The correct primer depends on substrate, adhesive chemistry, cleaning process, coating method, and drying requirements.

Accelerators

Accelerators are paired with specified LORD adhesive systems to initiate or influence cure behavior. Working time, production cycle, application sequence, and adhesive compatibility should be confirmed for the selected system.

Adhesion Promoters

Adhesion promoters and surface treatments improve receptivity of selected plastics, rubbers, and other difficult substrates when used with compatible bonding systems and the specified surface-preparation process.

Application Spotlight

EV Battery Packs

Parker LORD materials address several important interfaces within EV battery assemblies. LORD structural adhesives support bonded pack and module construction, while COOLTHERM materials provide options for thermal transfer, filling irregular interfaces, and potting or encapsulating selected components.

Thermal Heat-transfer materials
Bonding Structural adhesives
Interfaces Gap fillers & gels
Protection Potting & encapsulation
Explore the Application Page
EV battery pack application

Talk to our Experts

Krayden can help compare Parker LORD materials for structural bonding, thermal management, electronic assembly, elastomer bonding, surface preparation, and related manufacturing requirements. Our team can support product selection, substrate and application review, processing considerations, and comparison of candidate materials for your production needs.

Contact our team Call +1 (800) 448-0406

Parker LORD Quick Reference

Brands Carried
LORD, COOLTHERM, Chemlok
Core Technologies
Structural Bonding, Thermal Management, Electronic Packaging & Elastomer Bonding
Top Categories
Structural Adhesives, Thermal Management, Rubber-to-Substrate Bonding, Semiconductor Packaging
Key Markets
Aerospace & Defense, Transportation, EV & Electrification, Electronics & Semiconductors

164 products

  • LORD 7545 Two-Component Urethane Adhesive System

    LORD 7545 Two-Component Urethane Adhesive System

    • 1:1 mix ratio, 100% solids urethane adhesive
    • 1.5 to 65 minute selectable working time
    • Non-sag structural bonding with environmental and solvent resistance.
  • COOLTHERM EP 6972 KIT

    COOLTHERM EP 6972 KIT

    • <0.0005 ohm-cm Volume Resistivity
    • 2.13 W/(m K) Thermal Conductivity
    • 1:1 Weight Mixing
  • COOLTHERM 6053

    COOLTHERM 6053

    • Flexible Cured Material
    • Heat & Oxidation Resistance
    • Supplied in a 16-Ounce Aerosol Format
  • COOLTHERM 6250

    COOLTHERM 6250

    • 350 cP Low-Viscosity Curing Agent
    • High-Solids Adhesive/Encapsulation Curing Agent
    • Chemical-Resistant Cured Epoxy Systems
  • COOLTHERM 6732

    COOLTHERM 6732

    • Hardener Component Thermal Interface Material
    • 100:0.5 Controlled Mixing
    • Thermally Conductive Thermal Interface
  • COOLTHERM 6733

    COOLTHERM 6733

    • Solvent-Free RTV Silicone Encapsulation
    • Low-Stress No-Exotherm Room-Temperature Cure
    • -60 to 205 deg C Continuous Service
  • COOLTHERM EP-6010

    COOLTHERM EP-6010

    • 55 cP Application Viscosity
    • Low-Shrinkage Epoxy Curing Agent
    • Two-Year Shelf Life at 25 deg C
  • COOLTHERM MD-140

    COOLTHERM MD-140

    • 12 W/(m K) Thermal Conductivity
    • 72-Hour Working Window
    • Fast 120 to 180 deg C Cure
  • COOLTHERM PC10882

    COOLTHERM PC10882

    • Screen-Printable Coating Application
    • Thermal-Shock and Solvent-Resistant Cured Film
    • Above 500 V/mil Dielectric Strength
  • COOLTHERM SC-6730

    COOLTHERM SC-6730

    • Room-Temperature Thick-Section Cure
    • 3.0 to 10.0% Mix Concentration
    • Blue-Green Visual Mix Indicator
  • LORD 304-2

    LORD 304-2

    • High-Viscosity Placement Control
    • Rubber, Wood, and FRP Bonding
    • Durable Cured Performance with Environmental
  • LORD 306-2

    LORD 306-2

    • 306-1 Epoxy Hardener
    • 1 to 2-Hour Working Time
    • 24 to 48-Hour Room-Temperature Cure
  • LORD 4688

    LORD 4688

    • Low-Density Honeycomb-Core Syntactic Reinforcement
    • Thixotropic Application Control
    • 30-Minute Working Window
  • LORD 7100A

    LORD 7100A

    • High-Strength Structural Bonding
    • Primerless Bonding to Many Plastics
    • VOC-Free Weathering/Aging-Resistant Urethane
  • LORD 7100A/B

    LORD 7100A/B

    • High-Strength Structural Bonding
    • Without Priming Bonding
    • Solvent-, Weathering- and Aging-Resistant Cured System
  • LORD 7100B

    LORD 7100B

    • High-Strength Urethane Bonding
    • Primerless Bonding to Many Plastics
    • VOC-Free Weathering/Aging-Resistant Urethane
  • LORD 3135-B

    LORD 3135-B

    • Former Lord 7111-B Hardener
    • Low-Shrinkage Epoxy Bonding
    • Room-Temperature or Accelerated Heat Curing
  • LORD 7150A/B

    LORD 7150A/B

    • High-Strength Structural Bonding
    • Primerless Bonding to Many Plastics
    • Solvent-, Weathering- and Aging-Resistant Gray Cured System
  • LORD 7542A

    LORD 7542A

    • 1:1 Controlled Mixing
    • 4 to 30-Minute Working Window
    • 18.7 MPa Cured Tensile Strength
  • LORD 7542B

    LORD 7542B

    • 1:1 Fast-Cure Urethane Curative
    • 5 to 10-Minute Working Time
    • 30 to 60-Minute Handling Time
  • LORD 7542C

    LORD 7542C

    • 1:1 Medium-Work-Time Urethane Curative
    • 10 to 20-Minute Working Time
    • 60 to 120-Minute Handling Time
  • LORD 7545A/B

    LORD 7545A/B

    • Non-Sag Urethane Bonding
    • 3 to 5-Minute Working Window
    • 30-Minute Handling Time
  • LORD 7545A/D

    LORD 7545A/D

    • High-Strength Structural Bonding
    • Non-Sag Vertical Placement
    • Solvent and Weather Resistance
  • LORD 7550

    LORD 7550

    • Optically Clear Bonding
    • 3 to 5-Minute Working Window
    • Weathering/Humidity/Salt-Spray/UV Environmental Resistance
  • LORD 7650

    LORD 7650

    • One-Part Moisture-Cure Urethane
    • 15 to 30-Minute Solvent Flash
    • Multi-Material Foam/Fabric/Rubber/Plastic/Metal Bonding
  • LORD 7800

    LORD 7800

    • Rapid-Cure Urethane Bonding
    • Composite, SMC, Plastic, and Coated-Metal Bonding
    • Non-Sag Environmental Resistance
  • LORD ACCELERATOR 19GB

    LORD ACCELERATOR 19GB

    • Integrated 0.01 in (0.025 cm) Glass Beads
    • Room-Temperature Curing Paste Material
    • Non-Flammable Application Formulation
  • CHEMLOK 6411

    CHEMLOK 6411

    • 30-Minute Room-Temperature Dry
    • 12.7 to 25.4 um Film
    • Brush, Roll, Dip or Spray
  • COOLTHERM EP-6252

    COOLTHERM EP-6252

    • Defined Epoxy Hardener Component
    • Electrical Encapsulation System Use
    • Component-Level Metering Control
  • LORD 7542D

    LORD 7542D

    • Equal 1:1 Volume Mixing
    • 20-30 Minute Working Time
    • 70% Cured Elongation
  • COOLTHERM EP-6011

    COOLTHERM EP-6011

    • Hardener for Thermally Conductive Adhesive
    • EP-6006 HS System Pairing
    • Current-Carrying Conductor Bonding
  • COOLTHERM MT-125

    COOLTHERM MT-125

    • 2.35 W/(m K) Thermal Conductivity
    • 21 MPa Aluminum Lap Shear
    • Two-Week Working Life at 25 deg C
  • LORD 1110

    LORD 1110

    • Low-Density Epoxy Foam
    • Extended Working Time
    • High Compressive Strength
  • LORD 2232

    LORD 2232

    • 425 cP Application Viscosity
    • At Most 0.100 ohms/sq/mil Cured Resistivity
    • 2- to 3-Second Solder Wetting
  • LORD 307-2

    LORD 307-2

    • 20,000 to 57,000 cP Hardener Viscosity
    • 1:1 General-Purpose Volume Mix
    • 1- to 2-Hour System Working Time
  • LORD 312-B

    LORD 312-B

    • 0.96 g/cm^3 Hardener Density
    • 0.00% Volatile Content by Weight
    • Potting and Thin-Film Encapsulation
  • LORD 7411

    LORD 7411

    • 280-380% Cured Elongation
    • 1,000-5,000 cP at 82 deg C
    • Single-Component Moisture Cure
  • LORD 7433

    LORD 7433

    • 25-51 um Recommended Wet Film
    • 50,000-150,000 cP Viscosity
    • Single-Component Moisture Cure
  • LORD 7450

    LORD 7450

    • Cryogenic Flexible Bonding
    • Multifunction Adhesive and Sealant
    • Room-Temperature or Accelerated Cure
  • LORD 7545-A

    LORD 7545-A

    • Multi-Curative Work-Time Flexibility
    • Equal-Volume System Mixing
    • Manual or Automated Dispensing
  • LORD 7545-B

    LORD 7545-B

    • 3 to 5 Minute A/B Work Time
    • 30-Minute A/B Handling Strength
    • Non-Sag A/B Vertical Placement
  • LORD 7545-C

    LORD 7545-C

    • 6 to 8 Minute A/C Work Time
    • 60-Minute A/C Handling Strength
    • Non-Sag A/C Vertical Placement
  • LORD 7545D

    LORD 7545-D

    • 11 to 18 Minute A/D Work Time
    • 90-Minute A/D Handling Strength
    • Non-Sag A/D Vertical Placement
  • LORD 7545F

    LORD 7545F

    • 45 to 65 Minute A/F Work Time
    • Manual or Automated A/F Dispensing
    • Non-Sag A/F Vertical Placement
  • LORD 7555

    LORD 7555

    • Fast A/C Handling Strength
    • Extended 45-Minute A/E Work Time
    • Non-Sag Bead Placement
  • LORD 7556

    LORD 7556

    • Clear Plastic Bonding
    • Fast A/C Working Window
    • Non-Sag Cartridge Application
  • LORD 8621

    LORD 8621

    • Screen-Printable Resistor Paste
    • 90 to 110 Ohms/Square
    • 14 to 18 Micron Film
  • LORD PC-10678HV

    LORD PC-10678HV

    • Flexible-Substrate Screen Printing
    • Highly Conductive Grid Formation
    • One-Component Paste Processing
  • COOLTHERM ME-543

    COOLTHERM ME-543

    • 21,000 cP Jet-Dispense Viscosity
    • 7 to 20 Minute Cure at 160 to 165 deg C
    • 260 deg C Peak Reflow Resistance
  • LORD 410/19 GB 4:1 375ML

    LORD 410/19 GB

    • Acrylic Metal/Engineered-Plastic Structural Adhesive
    • 20 to 30-Minute Working Window
    • 18.6 MPa Cured Tensile Strength
  • ORD® 810S/20GB Flexible Acrylic Adhesive System

    LORD® 810S/20GB Flexible Acrylic Adhesive System

    • 2:1 mix ratio acrylic adhesive system
    • 8-12 minute selectable working time
    • Non-sag structural bonding with environmental and solvent resistance.
  • LORD SC-1600

    LORD SC-1600

    • 3.7 W/(m K) Conductivity
    • Equal 1:1 Meter-Mix Processing
    • 30-Minute Heat Cure
  • COOLTHERM SC-6754

    COOLTHERM SC-6754

    • 0.5 W/(m K) Thermal Conductivity
    • Nil Bleed After 24 Hours at 200 deg C
    • -55 to +205 deg C Continuous Service
  • COOLTHERM SC-3500

    COOLTHERM SC-3500

    • 3.5 W/(m K) Thermal Conductivity
    • <100 ppm Cyclic Siloxane Content
    • 1:1 Weight or Volume Mixing
  • COOLTHERM TC-404

    COOLTHERM TC-404

    • 4.3 W/(m K) Thermal Conductivity
    • 212,400 cP Viscosity
    • Reworkable Non-Curing Interface
  • COOLTHERM TC-501

    COOLTHERM TC-501

    • 25 to 50 um Installed Bondline
    • 3.6 W/(m K) Thermal Conductivity
    • 24-Hour Working Life at 25 deg C
  • COOLTHERM MG-121

    COOLTHERM MG-121

    • 2.3 W/(m K) Thermal Conductivity
    • Low-Modulus Cured Bonding
    • Eight-Hour Working Window
  • COOLTHERM MG-122

    COOLTHERM MG-122

    • Single-Component No-Mix Dispensing
    • Thermally Conductive Chip Interface
    • Flip-Chip and BGA Application Fit
  • COOTHERM CIRCALOK 6037

    COOTHERM CIRCALOK 6037

    • Thermally Conductive Bonding
    • 500,000 cP Resin Viscosity
    • 1.2 W/(m K) Thermal Conductivity
  • LORD 403

    LORD 403

    • LORD Accelerator 17/19/19GB Compatibility
    • Alternative to Welding/Brazing/Fastening
    • Acrylic Adhesive with Multiple Accelerators
  • LORD 403/19

    LORD 403/19

    • 2 to 4-Minute Working Window
    • Impact-Resistant Acrylic Bonding
    • Non-Sag Placement Control
  • LORD 406

    LORD 406

    • Medium-Work-Time Acrylic Adhesive
    • 6 to 10-Minute Working Window
    • 18.6 MPa Cured Tensile Strength
  • LORD 406/19GB

    LORD 406/19GB

    • 4:1 Metal-to-Plastic Bonding
    • 6 to 10-Minute Working Window
    • 18.6 MPa Cured Tensile Strength
  • LORD 506

    LORD 506

    • 4 to 6-Minute Working Window
    • Flexible Cured Adhesive
    • Environmental Resistance Acrylic Bonding
  • LORD 606/6

    LORD 606/6

    • Difficult Dcpd-Based FRP Bonding
    • 4 to 6-Minute Working Window
    • Glass-Bead Bondline Control
  • LORD 850S/25GB

    LORD 850S/25GB

    • Welding/Fastener Replacement Bonding
    • 6 to 10-Minute Working Time
    • Documented Chemical/Moisture/Salt-Spray/Weather Resistance
  • LORD 852/25GB

    LORD 852/25GB

    • Welding/Fastener Replacement Bonding
    • 20 to 25-Minute Working Time
    • Prepared/Unprepared Metal/FRP/Plastic Bonding
  • COOLTHERM 6403

    COOLTHERM 6403

    • 900 cP Mixed Viscosity
    • 45-Minute 25 deg C Cure
    • 50 to 120 deg C Service Range
  • COOLTHERM 6410

    COOLTHERM 6410

    • 600 cP Mixed Viscosity
    • Flexible Encapsulation Protection
    • Room-Temperature Encapsulation Cure
  • COOLTHERM 6712
  • COOLTHERM 6735

    COOLTHERM 6735

    • Eight-Hour Working Window
    • 55 to 205 deg C Service Range
    • Reversion-Resistant Addition-Cure System
  • COOLTHERM EP-343

    COOLTHERM EP-343

    • 1.1 W/(m K) Thermal Interface
    • 1 to 6 mil Spray Coats
    • 59 kV/mm Dielectric Strength
  • CHEMLOK 7701

    CHEMLOK 7701

    • Under Five-Minute Solvent Flash-Off
    • No-Mix Surface Conditioning
    • Wipe, Brush, Dip or Flood
  • COOLTHERM DC-812

    COOLTHERM DC-812

    • Automotive Encapsulation Application
    • 1.4 x 10^16 ohm-cm Volume Resistivity
    • Resistance to Thermal Shock and Electrical Stability
  • COOLTHERM E-105

    COOLTHERM E-105

    • Clear Unfilled Epoxy Resin
    • 600 cP Resin Viscosity
    • Multiple CoolTherm/Circalok Hardener Compatibility
  • CHEMLOK 607

    CHEMLOK 607

    • Clear One-Coat Silicone-Elastomer Bonding
    • Brush, Spray, or Dip Application
    • Extreme-Temperature Elastomer Bond Systems
  • COOLTHERM EP-2000

    COOLTHERM EP-2000

    • 1.9 W/(m K) Thermal Encapsulation
    • 1,900 cP Mixed Viscosity
    • 204 deg C Glass Transition
  • COOLTHERM EP-301

    COOLTHERM EP-301

    • 1.3 W/(m K) Thermal Encapsulation
    • High-Fluidity Intricate-Circuitry Potting
    • 19.7 kV/mm Dielectric Strength
  • COOLTHERM EP-340

    COOLTHERM EP-340

    • 1.5 W/(m K) Thermal Interface
    • 7,000 to 60,000 cP Mixed Viscosity
    • Low Cured Coefficient of Linear Thermal Expansion
  • COOLTHERM 6756

    COOLTHERM 6756

    • Adhesion-Promoting Surface Treatment
    • 1 cP Application Viscosity
    • Recommended 3 to 10 um Film Thickness
  • COOLTHERM EP-3500

    COOLTHERM EP-3500

    • 3.3 W/(m K) Thermal Conductivity
    • 10.4 to 12 ppm/deg C CTE
    • 205 to 206 deg C Glass Transition
  • COOLTHERM EP-6008

    COOLTHERM EP-6008

    • 8,000 cP Resin Viscosity
    • 1-Hour Working Window
    • 0.3 W/(m K) Thermal Interface
  • COOLTHERM EP-6009

    COOLTHERM EP-6009

    • 2,600 cP Mixed Viscosity
    • 0.7 W/(m K) Thermal Encapsulation
    • Electrically Insulating Encapsulation
  • COOLTHERM EP-6035

    COOLTHERM EP-6035

    • 1.0 W/(m K) Thermal Encapsulation
    • 12,000 cP Mixed Viscosity
    • UL 94 V-0 Classification
  • COOLTHERM EP-6037

    COOLTHERM EP-6037

    • 1.2 W/(m K) Thermal Conductivity
    • Two Hardener Options for Controlled CTE
    • Room-Temperature Adhesive Cure
  • COOLTHERM EP-636

    COOLTHERM EP-636

    • 205 deg C Staged-Cure Encapsulation
    • 18.3 kV/mm Dielectric Strength
    • 50,000 cP Mixed Viscosity
  • COOLTHERM ES-40

    COOLTHERM ES-40

    • Eight Configurable Hardener Options
    • Adhesive, Laminating, and Electrical-Insulation Uses
    • Up to 77.2 MPa Tensile Strength
  • COOLTHERM ME-525

    COOLTHERM ME-525

    • 6,000 cP High-Purity Capillary Underfill
    • 30-Minute 150 deg C Cure
    • 120 deg C Tg
  • COOLTHERM ME-531

    COOLTHERM ME-531

    • 4,000 cP Jettable Capillary Underfill
    • 140 deg C Glass Transition
    • 30-Minute 150 deg C Cure
  • COOLTHERM SC-104

    COOLTHERM SC-104

    • 0.8 W/(m K) Thermal Encapsulation
    • 7,000 cP Mixed Viscosity
    • 17.3 kV/mm Dielectric Strength
  • LORD 310

    LORD 310

    • Thixotropic Application Control
    • 30 to 60-Minute Working Window
    • 32 MPa Cured Tensile Strength
  • COOLTHERM SC-303

    COOLTHERM SC-303

    • 0.9 W/(m K) Thermal Conductivity
    • 6,000 cP Application Viscosity
    • 40 to 200 deg C Service Range
  • COOLTHERM SC-6702

    COOLTHERM SC-6702

    • 0.7 W/(m K) Silicone Encapsulation
    • 4-Hour Working Life
    • -55 to 260 deg C Material Use
  • COOLTHERM SC-6703

    COOLTHERM SC-6703

    • 0.8 W/(m K) Thermal Encapsulation
    • 8,000 cP Mixed Viscosity
    • 19.7 kV/mm Dielectric Strength
  • COOLTHERM SC-6705

    COOLTHERM SC-6705

    • 55 to 205 deg C Service Range
    • 2,500 cP Mixed Viscosity
    • 17.7 kV/mm Dielectric Strength
  • COOLTHERM SC-6709

    COOLTHERM SC-6709

    • 1.0 W/(m K) Thermal Encapsulation
    • Three Hardener Options
    • 68 to 205 deg C Service Range
  • COOLTHERM SC-6710

    COOLTHERM SC-6710

    • 1.0 W/(m K) Thermal Encapsulation
    • 20,000 cP Red Resin with Sc-6730 Processing
    • 19.7 kV/mm Dielectric Strength
  • COOLTHERM SC-6711

    COOLTHERM SC-6711

    • 1.0 W/(m K) Thermal Encapsulation
    • 30,000 cP White Silicone Resin
    • 19.7 kV/mm Dielectric Strength
  • COOLTHERM SC-6714

    COOLTHERM SC-6714

    • UL 94 V-0 Encapsulation
    • 55 to 205 deg C Service Range
    • Circalok 6730/6731 Catalyst Compatibility
  • COOLTHERM SC-6725

    COOLTHERM SC-6725

    • 1.16 W/(m K) Thermal Encapsulation
    • 15,000 cP Mixed Viscosity
    • Primerless Encapsulation Processing
  • COOLTHERM SC-6731

    COOLTHERM SC-6731

    • 100 cP Resin Viscosity
    • Concentrations from 0.1% to 5% by Weight
    • Two-Component RTV Silicone Systems Used in Potting
  • COOLTHERM UR388

    COOLTHERM UR388

    • 0.7 W/(m K) Thermal Encapsulation
    • 6,000 cP Mixed Viscosity
    • 0.32% TML and 0.02% CVCM
  • LORD 406E

    LORD 406E

    • High-Impact and Peel Performance
    • 6-10 Minute Working Time
    • Minimal Metal Surface Preparation
  • LORD 410/19GB

    LORD 410/19GB

    • Glass-Bead Bondline Control
    • 20-30 Minute Working Time
    • Non-Sag Vertical Application
  • COOLTHERM SC-309

    COOLTHERM SC-309

    • 0.9 W/(m K) Thermal Encapsulation
    • Low-Viscosity Automated Meter-Mix Processing
    • Room- or Heat-Cure Flexibility
  • LORD MAXLOK MX/T3S

    LORD MAXLOK MX/T3S

    • Minimal-Preparation Metal Bonding
    • Fast 6- to 8-Minute Handling
    • Controlled Non-Sag Bondline
  • COOLTHERM MT-322

    COOLTHERM MT-322

    • 1.7 W/(m K) Thermal Conductivity
    • One-Month Working Life at 25 deg C
    • -40 to +200 deg C Service Range
  • LORD 459X

    LORD 459X

    • Adhesion-Promoting Surface Treatment
    • Low-Viscosity Adhesive Application
    • Brush, Dip or Spray Application
  • LORD 7701

    LORD 7701

    • Cured-Rubber/Urethane/Elastomer Adhesion Treatment
    • No-Mix Wipe/Brush/Dip/Flood Application
    • Compatible LORD Epoxy/Urethane Adhesives
  • LORD AP-134

    LORD AP-134

    • One-Coat Moisture-Cure Multi-Substrate Primer
    • No-Mix Spray/Dip/Felt Application
    • 1 to 2-Hour Ambient Hydrolysis
  • LORD P-1291

    LORD P-1291

    • Low-Viscosity Brush or Spray
    • Metal and Glass Adhesion Promotion
    • 30 to 60 Minute Air-Dry
  • LORD P-1292

    LORD P-1292

    • Platinum-Cure RTV Adhesion Promotion
    • Broad-Substrate Addition-Cure Silicone Adhesion
    • Hydrolytically Stable Silicone Bonding
  • COOLTHERM EP-6007

    COOLTHERM EP-6007

    • 45-Minute Working Window
    • 0.62 W/(m K) Thermal Interface
    • 19.7 kV/mm Dielectric Strength
  • CoolTherm® SC-320 Thermally Conductive Silicone

    CoolTherm® SC-320 Thermally Conductive Silicone

    • 3.0 W/m·K thermal conductivity
    • Low-stress, low-viscosity silicone
    • UL 94 V-0 and Class H insulation
  • CoolTherm® SC-324 Thermally Conductive Silicone

    CoolTherm® SC-324 Thermally Conductive Silicone

    • 4.0 W/m·K thermal conductivity
    • Durable UL 94 V-0 flame rated, addition-cure PDMS
    • Low-stress low viscosity potting
  • COOLTHERM 6055

    COOLTHERM 6055

    • Convenient 1:1 Volume Mixing
    • Room-Temperature or Accelerated Cure
    • Dielectric Epoxy Encapsulation
  • COOLTHERM 6408

    COOLTHERM 6408 6408 A SLW/B

    • Extended 20-30 Minute Work Life
    • High-Elongation Cured Protection
    • Electrical Insulation for Encapsulation
  • COOLTHERM 6715

    COOLTHERM SC-6715

    • Multiple Hardener Pairing Options
    • Automatic Meter-Mix-Dispense Application
    • Dense-Component Potting Resin
  • COOLTHERM 6716

    COOLTHERM 6716

    • 45-Minute Mixed Working Window
    • 100:2.5 Resin-Hardener Ratio
    • Low- and High-Voltage Encapsulation
  • COOLTHERM 6744

    COOLTHERM 6744

    • Low-Viscosity 1:1 Processing
    • Two-Hour Room-Temperature Cure
    • Flame-Retardant Silicone Encapsulation
  • COOLTHERM EP-6028

    COOLTHERM EP-6028

    • 1:1 Resin-Hardener Mixing
    • High-Voltage Transformer Potting
    • 3-4 Hour System Heat Cure
  • COOLTHERM ES-21

    COOLTHERM ES-21

    • 35,000 cP Dispensing Viscosity
    • UV Fluorescence for In-Line Inspection
    • 60-Minute Cure at 125 deg C
  • COOLTHERM SC-252

    COOLTHERM SC-252

    • 2.5 W/(m K) Thermal Conductivity
    • 8.7 kV/mm Dielectric Strength
    • 1:1 Weight or Volume Mixing
  • COOLTHERM SC-420

    COOLTHERM SC-420

    • 3.2 W/(m K) Thermal Conductivity
    • 100% Cured Elongation
    • 2:1 Weight or Volume Mixing
  • COOLTHERM SC-6709/SC-6731

    COOLTHERM SC-6709/SC-6731

    • 100:0.5 Weight Mixing
    • 12 to 16 Hour Room-Temperature Cure
    • 21.7 kV/mm Dielectric Strength
  • COOLTHERM SC-6717

    COOLTHERM SC-6717

    • 17,000 cP Resin Viscosity
    • 8 to 24 Hour Room-Temperature Cure
    • 19.7 kV/mm Dielectric Strength
  • COOLTHERM SC-6726

    COOLTHERM SC-6726

    • 3 to 5 Day Working Life at 25 deg C
    • 1:1 Weight or Volume Mixing
    • -55 to +200 deg C Operating Range
  • COOLTHERM UR-288

    COOLTHERM UR-288

    • 100:20 Weight Mixing
    • 30-Minute Working Time at 25 deg C
    • UL 94 HB at 3.0 mm
  • COOLTHERM UR-388

    COOLTHERM UR-388

    • UL 94 V-0 Classification
    • 0.7 W/(m K) Thermal Conductivity
    • 15.0 kV/mm Dielectric Strength
  • LORD 201/17

    LORD 201/17

    • 10:1 Volume Mix Ratio
    • 5- to 8-Minute Working Time
    • 31.7 MPa 6061-T6 Aluminum Lap Shear
  • LORD 406/17

    LORD 406/17

    • 10:1 Accelerator 17 Volume Mix
    • 6-10 Minute Working Window
    • 12-17 Minute Handling Strength
  • LORD 410

    LORD 410

    • 20-30 Minute Working Window
    • 0.25 mm 19GB Bondline Control
    • 4:1 Volume System Mixing
  • LORD 506/17

    LORD 506/17

    • 8-12 Minute Handling Strength
    • 10:1 Accelerator 17 Volume Mix
    • -40 to 149 deg C Temperature Range
  • LORD 606

    LORD 606

    • 5-7 Minute Mixed Working Window
    • 10:1 Accelerator 17 Volume Mix
    • DCPD Composite-to-Metal Bonding
  • LORD 661/6

    LORD 661/6

    • Up to 25.4 mm Gap Fill
    • 11-19 Minute Working Window at 32 deg C
    • 45-55 Minute Handling Strength
  • LORD 810

    LORD 810

    • Low Read-Through Bondline
    • Thin-Gauge Panel Bonding
    • 2:1 Volume Mixing
  • LORD 810S

    LORD 810S

    • Minimal Bond-Line Read-Through
    • 8 to 12 Minute Work Time
    • -40 to 300 deg F Range
  • LORD RT8

    LORD RT8

    • 800 to 1000 cP Flowability
    • Low-Exotherm Potting Systems
    • Large-Casting Encapsulation Fit
  • LORD MAXLOK T18S

    LORD MAXLOK T18S

    • 18 to 24 Minute Work Time
    • 48 to 72 Minute Handling
    • -40 to 300 deg F Range
  • LORD MAXLOK T3S

    LORD MAXLOK T3S

    • 3 to 5 Minute Work Time
    • 6 to 8 Minute Handling
    • Non-Sag Structural Placement
  • LORD MAXLOK T6S

    LORD MAXLOK T6S

    • 6 to 9 Minute Work Time
    • 20 to 24 Minute Handling
    • Exact MX/T6S Cured Data
  • LORD 2850

    LORD 2850

    • 62.1 MPa Compressive Strength
    • Low-Outgassing 0.01% CVCM
    • Trowel or Injection Application
  • LORD 304-1

    LORD 304-1

    • High-Viscosity Placement Control
    • Rubber, Wood, and FRP Bonding
    • Durable Cured Performance with Environmental
  • LORD 305-1

    LORD 305-1

    • Medium-Viscosity Application Control
    • Rubber-to-Wood Epoxy Bonding
    • Chemically, Environmentally and Temperature Resistant
  • LORD 305-1/2

    LORD 305-1/2

    • Medium-Viscosity Application Control
    • Rubber-to-Wood Epoxy Bonding
    • Chemically, Environmentally and Temperature Resistant
  • LORD 305-2

    LORD 305-2

    • Medium-Viscosity Application Control
    • Rubber-to-Wood Epoxy Bonding
    • Chemically, Environmentally and Temperature Resistant
  • LORD 306-1

    LORD 306-1

    • High-Viscosity Non-Sag Gap Filling
    • Documented Chemical/Moisture/Weather Resistance
    • MIL-A-24456 Compliance Scope
  • LORD 3135

    LORD 3135

    • Broad Multi-Material Structural Bonding
    • Low-Shrinkage Epoxy System
    • Documented NASA/MMM-A-134/MIL-A-8623A Compliance
  • LORD 3170

    LORD 3170

    • Bond Strength Down to -253 deg C
    • Low-Outgassing Aerospace Epoxy
    • Equal-Volume Room-Temperature Cure
  • LORD 320

    LORD 320

    • Primerless Automotive-SMC Adhesion
    • -40 to 204 deg C Service Range
    • Solvent-Free Nonflammable Epoxy
  • LORD 320/310B-BLK

    LORD 320/310B

    • Two-Component Epoxy for Treated Cured Rubber
    • 30 to 60-Minute Working Window
    • Durability Under Humidity Bonding
  • LORD 320/322

    LORD 320/322

    • Primerless Automotive-SMC Adhesion
    • -40 to 204 deg C Service Range
    • Solvent-Free Nonflammable Epoxy
  • LORD 322

    LORD 322

    • General-Purpose Two-Component Epoxy for SMC
    • 20 to 40-Minute Working Window
    • 30.6 MPa Cured Tensile Strength
  • LORD 363

    LORD 363

    • 3 to 5-Minute Working Window
    • Self-Leveling Flowable Placement
    • Solvent-Free Bonding Formulation
  • CHEMLOK 485

    CHEMLOK 485

    • One-Month Mixed Working Life
    • 17.8 to 25.4 um Film
    • Spray, Brush or Dip Application
  • LORD 312-A

    LORD 312-A

    • 1.13 g/cm^3 Resin Density
    • 0.00% Volatile Content by Weight
    • Potting and Thin-Film Encapsulation
  • LORD 7550A Urethane Adhesive

    LORD 7550A Urethane Adhesive

    • Equal-Mix LORD 7550 Resin Component
    • 1,800 to 4,000 cP Viscosity
    • Lexan, ABS, and Primed-Metal Bonding
  • LORD 7550C Urethane Adhesive

    LORD 7550C Urethane Adhesive

    • Equal-Mix LORD 7550 Curative Component
    • 6,000 to 12,500 cP Viscosity
    • Lexan, ABS, and Primed-Metal Bonding
  • LORD 309-1D

    LORD 309-1D

    • Non-Sag Vertical Bonding
    • 1.5-2 Hour Work Time
    • Room- or Heat-Cure Flexibility
  • COOLTHERM 6027

    COOLTHERM 6027

    • Fast Heat-Cure Processing
    • Non-Sag Thixotropic Dispensing
    • High-Resistivity Cured Insulation
  • COOLTHERM EP-6151

    COOLTHERM EP-6151

    • Thermally Conductive Heat-Sink Bonding
    • Fast High-Temperature Cure
    • Shape-Holding Thixotropic Dispensing
  • LORD 320/323

    LORD 320/323

    • 20-40 Minute Working Window
    • 45-60 Minute Cure at 82 deg C
    • UV-Fluorescent Mix Inspection
  • LORD 360

    LORD 360

    • 1:1 Equal-Volume Mixing
    • 5-10 Minute Handling Strength
    • Minimal-Sag Vertical Application
  • LORD EX-5640

    LORD EX-5640

    • Controlled Non-Slump Flow
    • Electronics Structural Bonding
    • Thermal and Dielectric Data

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers