COOLTHERM EP-6151
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Thermally Conductive Heat-Sink Bonding
- Fast High-Temperature Cure
- Shape-Holding Thixotropic Dispensing
Product Description
CoolTherm EP-6151 Epoxy Adhesive is a one-component, aluminum-filled epoxy used as a thermal-interface adhesive for heat-sink attachment and related bonding applications. The gray paste has a typical viscosity of 750,000 cP at 25 deg C and thixotropic, non-sag rheology that maintains dispensed shape. The cure schedule is 30 minutes at 121 deg C or 10 minutes at 177 deg C. Typical cured properties include 0.6 W/(m K) thermal conductivity, a 124 deg C glass transition temperature by TMA, and Shore D 90 hardness. Its operating temperature range is -40 to +150 deg C.
Key features
- Thermally Conductive Bondline: Typical cured thermal conductivity is 0.6 W/(m K) for heat-transfer bonding applications.
- Rapid Heat Cure: Cures in 30 minutes at 121 deg C or 10 minutes at 177 deg C after the adhesive reaches temperature.
- Shape-Holding Dispensing: Thixotropic rheology maintains the dispensed adhesive shape before cure.
Applications
Thermal-interface and heat-sink attachment where a thermally conductive epoxy adhesive is required.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Additional Information
As-Supplied Properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Gray paste | Typical; uncured | |
| Viscosity | 750,000 | cP | Typical; uncured; 25 deg C |
| Specific gravity | 1.50 | Typical; uncured |
Final-State Properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Thermal conductivity | 0.6 | W/(m K) | Typical; cured |
| Glass transition temperature (Tg) | 124 | deg C | Typical; cured; TMA |
| Hardness | 90 | Shore D | Typical; cured; 25 deg C |
| Tensile strength | 3000 | psi | Typical; cured; AL-AL |