COOLTHERM 6716
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- 45-Minute Mixed Working Window
- 100:2.5 Resin-Hardener Ratio
- Low- and High-Voltage Encapsulation
Product Description
Circalok 6716 Silicone Resin is the resin component of a two-component, solvent-free RTV silicone system used with Circalok 6733 hardener. The black liquid has a typical viscosity of 10,000 cP and specific gravity of 1.40 at 25 deg C. When combined with Circalok 6733 hardener, the resin and hardener mix at 100:2.5 by weight, provide a typical 45-minute working life at 25 deg C, and cure in 12 to 16 hours at 25 deg C. The system is used for potting and encapsulating both low- and high-voltage electrical and electronic assemblies.
Key features
- 6733 Hardener Pairing: Circalok 6716 resin is formulated for use with Circalok 6733 hardener.
- 45-Minute Working Life: The 6716/6733 mixed system has a typical 45-minute working life at 25 deg C.
- Electrical Assembly Encapsulation: The 6716/6733 system is used for potting low- and high-voltage electrical and electronic assemblies.
Applications
Resin component for the Circalok 6716/6733 silicone system used to pot and encapsulate low- and high-voltage electrical and electronic assemblies.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Electrical Properties
Thermal Properties
Mechanical Properties
Additional Information
As-Supplied Properties
Values apply to the Circalok 6716 resin component as supplied.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Black liquid | Typical; 6716 resin | |
| Viscosity | 10,000 | cP | Typical; 6716 resin; 25 deg C |
| Specific gravity | 1.40 | Typical; 6716 resin; 25 deg C |