COOLTHERM EP-6011
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Hardener for Thermally Conductive Adhesive
- EP-6006 HS System Pairing
- Current-Carrying Conductor Bonding
Product Description
CoolTherm EP-6011 Hardener is the hardener component used with CoolTherm EP-6006 HS resin to form the two-component EP-6006 HS/6011 epoxy adhesive system. It is supplied as an amber liquid with a typical density of 1.22 g/cm^3 and is insoluble in water. The paired system is used as a thermally conductive adhesive for bonding current-carrying conductors. EP-6011 must be combined with EP-6006 HS resin to form the adhesive; the hardener alone is not the cured bonding material.
Key features
- EP-6006 HS Pairing: EP-6011 pairs with EP-6006 HS resin in the two-component adhesive system.
- Liquid Hardener Form: The hardener is an amber liquid with a typical density of 1.22 g/cm^3.
- Conductor Bonding System: The paired EP-6006 HS/6011 system is used for thermally conductive bonding of current-carrying conductors.
Applications
Hardener component for the EP-6006 HS/6011 thermally conductive epoxy adhesive system used to bond current-carrying conductors.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-Supplied Properties
Values apply to the EP-6011 hardener component as supplied.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Amber | Typical; EP-6011 hardener | |
| Physical state | Liquid | Typical; EP-6011 hardener | |
| Density | 1.22 | g/cm^3 | Typical; EP-6011 hardener |
| Water solubility | Insoluble | Typical; EP-6011 hardener |