PLEXUS MA2230

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PLEXUS MA2230/2245/MA2290

Main features

  • 40-42 Minute Work Time
  • Highly Thixotropic 10:1 Adhesive Family
  • 0.75-38 mm Grade-Specific Gaps

Product Description

Plexus MA2230 is a highly thixotropic two-part methacrylate structural adhesives for thermoplastic, metal and composite assemblies. Each grade uses a 10:1 mix ratio and retains its own processing and cured-property data. At 23.9 deg C, typical work time is 40-42 minutes. It lists a gap tolerance from 0.75 to 38 mm.

  • Three grade-specific work-time options: At 23.9 deg C, MA2230 is 40-42 minutes
  • 10:1 two-part methacrylate systems
  • 0.75-38 mm grade-specific gap tolerance

Applications

Structural bonding of composites, thermoplastics and metals; large-bead and vertical assemblies where the selected grade's work time and technical data support use.

Technical Specifications

General Properties
Color
The color
Off-White/Black
Density (g)
0.99/1.07 g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
10:1
Physical Properties
Viscosity (Part A)
190 - 250 mPa.s
Viscosity (Part B)
35 - 70 mPa.s

Leading Brands Trust in Our Products and Services