PERMABOND LH197
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Flexible Flange Gasketing for Dissimilar Metals
- Low-Strength Gasket for Routine Disassembly
- Formed-In-Place Sealing for Soft-Metal Surfaces
Product Description
Permabond LH197 is a flexible anaerobic formed-in-place gasket maker for metal flange surfaces, including dissimilar and soft-metal assemblies. The material forms a gasket between mating metal surfaces and is intended for applications where differential thermal expansion or routine disassembly makes a flexible, lower-strength gasket useful. It fills gaps up to 0.3 mm and reaches typical handling strength on M10 steel in 20 minutes at 23 deg C. Typical cured shear strength is 5 MPa on a steel collar-and-pin test to ISO 10123. LH197 can be dismantled with normal tools for flange assemblies that require periodic disassembly.
Key features
- Flexible formed-in-place gasketing: Forms a flexible gasket between mating metal surfaces.
- Dissimilar and soft-metal flanges: Designed for dissimilar surfaces and soft metals where differential thermal expansion or damage during disassembly can matter.
- Routine disassembly with normal tools: The cured gasket can be dismantled with normal tools for assemblies requiring periodic access.
Applications
Formed-in-place gasketing of metal flanges; dissimilar-metal flange sealing; soft-metal surfaces and assemblies requiring routine disassembly.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Electrical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical composition | Acrylic | - | Uncured material |
| Viscosity | 50,000 at 2 rpm; 20,500 at 20 rpm | cP | Uncured material; 25 deg C |
| Specific gravity | 1.1 | - | Uncured material |
| Storage temperature | 5 to 25 | deg C | Manufacturer storage guidance |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Break torque | 10 | N m | Typical cured material; M10 steel; ISO 10964 |
| Prevailing torque | 5 | N m | Typical cured material; M10 steel; ISO 10964 |
| Shear strength | 5 | MPa | Typical cured material; steel collar and pin; ISO 10123 |