PERMABOND ET5429

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND ET5429

Main features

  • Composite-Focused Structural Bonding
  • 6 to 10 Hour Handling Window
  • Thixotropic Vertical Gap Filling

Product Description

PERMABOND ET5429 is a thixotropic two-component epoxy adhesive for composite bonding and gap-filling structural assembly. It is supplied as a thixotropic paste, with a handling time of 6 to 10 hours at 23 deg C and shear strength of 23 to 28 MPa. The extended handling window provides substantial time for positioning large or complex assemblies before handling strength develops. Applications include composite assembly, vertical or gap-filling bonds and structural joints where impact or vibration resistance and elevated-temperature capability are required. The paste rheology and long working profile suit composite-focused assembly processes that need controlled placement across larger bond areas.

Key features

  • Composite-Bonding Epoxy: Primary applications include composite assembly and structural bonding.
  • 6 to 10 Hour Handling: Long handling time at 23 deg C provides more time for large or complex assembly workflows.
  • Thixotropic Gap Fill: Paste rheology provides controlled placement for vertical and gap-filling bonds.

Applications

Composite assembly, gap-filling or vertical bonding and structural applications requiring impact or vibration resistance and elevated-temperature capability.

Product Family

PERMABOND ET5429

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White/Black
Chemistry Type
Epoxy Resin/Polyamine Hardener
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
2:1
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.0
Physical Properties
Viscosity (Part A)
200,000 mPa.s
Viscosity (Part B)
60,000 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
5 %
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
50-60 °C
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
15-25 kV/mm

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers