PERMABOND ET500

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND ET500

Main features

  • 5 to 8 Minute Handling
  • Clear Rapid-Cure Epoxy Bonding
  • 12 to 18 MPa Shear

Product Description

PERMABOND ET500 is a clear, two-component epoxy adhesive for rapid structural assembly. Viscosity is 13,000 to 24,000 mPa s, handling time is 5 to 8 minutes at 23 deg C, and shear strength is 12 to 18 MPa. The fast handling profile suits smaller or time-sensitive bonding operations where a clear epoxy is preferred. Applications include bonding wood, metals, ceramics, selected plastics and composites. The resin-and-hardener format provides a structural epoxy bond for multi-material joints while keeping the assembly window short enough for rapid production steps and quick transition from placement to handling.

Key features

  • 5 to 8 Minute Handling: Handling time is 5 to 8 minutes at 23 deg C for rapid assembly workflows.
  • Clear Two-Part Epoxy: The product is a clear epoxy resin and hardener system for structural bonding.
  • 12 to 18 MPa Shear: Shear strength is 12 to 18 MPa.

Applications

Bonding wood, metals, ceramics, selected plastics and composites in small or rapid assembly applications.

Product Family

PERMABOND ET500

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Colourless
Chemistry Type
Epoxy Resin/Amine Hardener
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:1
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Physical Properties
Viscosity (Part A)
12,000-18,000 mPa.s
Viscosity (Part B)
15,000-30,000 mPa.s
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
15-25 kV/mm
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.22 W/m.K

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers