MOLYKOTE P-1500
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses
Main features
- Assembly and Long-Term Lubrication
- Heavy-Load Sliding Contact Protection
- Wide-Temperature Metallic Component Use
Product Description
MOLYKOTE P-1500 Paste is a white semi-synthetic grease-paste with lithium soap, solid lubricants, and a corrosion inhibitor for assembly and long-term lubrication of metallic components. Its service-temperature range extends from -50 to 160 deg C. At 40 deg C, the base oil has a typical viscosity of 90 mm^2/s, while the four-ball weld load is 4,000 N. Water resistance and anti-fretting behavior support heavily loaded sliding contacts at low to medium speeds. Application methods include brush, grease gun, and central lubrication systems across electrical appliances, precision instruments, machinery, and automotive components.
Key features
- Assembly and Long-Term Use: The grease-paste is intended for metallic-component assembly and extended lubrication.
- Wide Service-Temperature Range: The typical service range extends from -50 to 160 deg C.
- Heavy-Load Contact Performance: Typical four-ball weld load is 4,000 N, with water resistance and anti-fretting performance in testing.
Applications
Metallic-component assembly, heavily loaded sliding contacts, electrical and domestic appliances, precision instruments, machinery, and automotive components.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | White | - | Typical value |
| Unworked penetration | 290 to 320 | mm/10 | ISO 2137; typical value |
| Density | 1.05 | g/ml | ISO 2811; 20 deg C; typical value |
| Base-oil viscosity | 90 | mm^2/s | DIN 51562; 40 deg C; typical value |
| Dropping point | 170 | deg C | ISO 2176; typical test result; not a service-temperature limit |