MOLYKOTE MI-60

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE MI60

Main features

  • Plastic-Compatible Long-Term Lubrication
  • Wide-Temperature Mechanical Lubrication
  • High-Load Grease Performance

Product Description

MOLYKOTE MI-60 (USA) Grease is a light-consistency synthetic hydrocarbon grease thickened with lithium soap and formulated with solid lubricants for long-term lubrication of mechanical and automotive elements. Its useful temperature range is -50 to 150 deg C, and typical four-ball results are a 0.45 mm wear scar after 1 hour at 400 N and a 4,300 N EP OK load. The grease is compatible with polyacetal, polyamide, PS foam, and nylon, and it can be applied by brush, grease gun, or automatic dispensing for steering columns, ignition mechanisms, and servo motors.

Key features

  • Plastic-Compatible Formulation: The grease is compatible with polyacetal, polyamide, PS foam, and nylon.
  • Wide Useful Temperature Range: The typical useful range extends from -50 to 150 deg C.
  • Load and Wear Performance: Typical four-ball results include a 0.45 mm wear scar at 400 N and a 4,300 N EP OK load.

Applications

Long-term lubrication of steering columns, ignition mechanisms, servo motors, and other mechanical or automotive elements.

Technical Specifications

General Properties
Color
The color
Yellow

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorYellow-Typical value
Worked penetration300mm/10Worked 60; typical value
NLGI grade1 to 2UnitlessTypical value
Dropping point195deg CTypical test result; not a service-temperature limit