MOLYKOTE G-807

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE G-807

Main features

  • Low-Friction Electromechanical Lubrication
  • Plastic and Rubber Compatibility
  • -40 to 150 deg C Range

Product Description

MOLYKOTE G-807 Low Friction Silicone Compound is a soft, white NLGI 1 silicone compound modified with PTFE solid lubricants for low-friction electromechanical contacts. It is intended primarily for plastic-to-metal and metal-to-rubber lubrication, including automotive ball joints and brake-caliper pins. The compound carries a useful temperature range of -40 to 150 deg C and combines plastic and rubber compatibility with corrosion resistance. Typical properties include 300 unworked penetration, 1.146 specific gravity, 0.5% maximum bleed and 1.0% maximum evaporation under the stated 150 deg C test conditions.

Key features

  • Low-friction electromechanical lubrication: Supports plastic-to-metal and metal-to-rubber contacts in supported electromechanical assemblies.
  • Plastic and rubber compatibility: Fits supported polymer and elastomer interfaces within the specified application limits.
  • -40 to 150 deg C range: Carries a useful temperature range for automotive and related supported contact points.

Applications

Applications include automotive ball joints, brake-caliper pins and supported plastic-to-metal or metal-to-rubber electromechanical interfaces.

Product Family

MOLYKOTE G-807

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.146

Additional Information

Technical properties

As-supplied / before-processing properties

Typical bulk-compound values apply before installation or service exposure.

PropertyValueUnitMethod / condition
ColorWhite-Typical; as supplied
Consistency1NLGI gradeManufacturer product details
Thickener / solid lubricantPTFE-Manufacturer product details
Unworked penetration3000.1 mmTypical; source method not stated
Specific gravity1.146-Typical; source temperature not stated
Usable life60monthsOriginal closed container at ambient temperature
Technical properties

After-processing / final-state properties

In-service and accelerated-test values remain limited to the stated conditions.

PropertyValueUnitMethod / condition
Useful temperature range-40 to 150deg CInstalled or in-use compound
Bleed0.5 maximum%24 hours at 150 deg C
Evaporation1.0 maximum%24 hours at 150 deg C
Melting pointNone-Typical manufacturer result