MOLYKOTE G-1041

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE G-1041

Main features

  • Plastic-Compatible Synthetic Lubrication
  • -60 deg C Low-Temperature Operation
  • Low-Evaporation PAO Grease

Product Description

MOLYKOTE G-1041 Grease is a beige PAO-based lithium grease for gears, actuators and bearings in supported plastic-to-plastic, plastic-to-metal and metal-to-metal contacts under low to medium loads. Its service-temperature range is -60 to 130 deg C, supporting selection for low-temperature mechanisms. Typical properties include 280 worked penetration, 2% bleed, less than 1% evaporation, and a 0.6 mm four-ball wear scar under the stated test conditions. The grease may be applied by brush, spatula or automated equipment after contact points are cleaned.

Key features

  • Plastic-compatible synthetic lubrication: Lubricates supported plastic and mixed-material gears, actuators and related sliding contacts.
  • -60 deg C low-temperature operation: Has this lower service-temperature limit for supported mechanisms.
  • Low-evaporation PAO grease: Has less than 1% evaporation under the specified test condition.

Applications

Applications include supported gears, actuators and bearings using plastic-to-plastic, plastic-to-metal or metal-to-metal contacts under low to medium loads.

Product Family

MOLYKOTE G-1041

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Beige

Additional Information

Technical properties

As-supplied / before-processing properties

Typical bulk-grease and test values are shown separately from the documented -60 to 130 deg C service-temperature range.

PropertyValueUnitMethod / condition
ColorBeige-Typical; as supplied
Worked penetration2800.1 mmTypical; 60 strokes
Dropping point210deg CTypical; not an operating-temperature limit
Bleed2%Typical; manufacturer test condition
Evaporation<1%Typical; manufacturer test condition
Copper corrosion1aratingTypical; manufacturer test condition
Four-ball wear scar0.6mmTypical; 1,200 rpm, 75 deg C, 1 hour
Low-temperature torque45 starting / 12 runningmN-mTypical at -40 deg C