MOLYKOTE AI-6159 Grease is a white PAO-based lithium grease containing PTFE and additives for lubrication and noise control in automotive plastic sliding components. Applications include window-regulator guides and other supported sliding parts. The grease has a service-temperature range of -40 to 150 deg C and may be applied by brush, spatula or automated equipment. Typical properties include 305 worked penetration, 1.9% bleed after 24 hours at 100 deg C, and a 0.61 mm four-ball wear scar under the stated test conditions.
Key features
- Automotive plastic noise control: Supports lubrication and noise reduction in supported automotive plastic sliding components.
- Window-regulator guide lubrication: Fits window-regulator guides and other supported sliding parts in automotive assemblies.
- -40 to 150 deg C range: Has this service-temperature range for the supported applications.
Applications
Applications include automotive window-regulator guides and other supported plastic sliding components requiring lubrication and noise reduction.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Typical grease and test values apply to MOLYKOTE AI-6159 Grease under the stated conditions.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | White | - | Typical; as supplied |
| Worked penetration | 305 | 0.1 mm | Typical; 60 strokes |
| Bleed | 1.9 | % | Typical; 24 hours at 100 deg C |
| Evaporation | 0.2 | % | Typical; 22 hours at 99 deg C |
| Four-ball wear scar | 0.61 | mm | ASTM D2266; 1,200 rpm, 392 N, 1 hour |
| Copper corrosion | 1a | rating | Typical; 24 hours at 100 deg C |
| Low-temperature starting torque | 290 | mN-m | Typical at -40 deg C |
| Low-temperature running torque | 130 | mN-m | Typical at -40 deg C |