LOCTITE SI 5050
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.
Main features
- Less Than 3.00% VOC Content
- Approximately 1.0 Specific Gravity
- Translucent Liquid or Paste Form
Product Description
LOCTITE SI 5050 is a one-part light-curing silicone sealant and adhesive supplied as a translucent liquid or paste. The as-supplied material has a slight odor, approximate specific gravity of 1.0, VOC content below 3.00%, slight water solubility, and vapor pressure below 5 mm Hg at 20 deg C. Its boiling point and flash point are both above 93 deg C. These technical values describe only the as-supplied material and do not define cure behavior or bonded performance.
Key features
- As-Supplied VOC Limit: VOC content is less than 3.00%.
- As-Supplied Density: Approximate specific gravity is 1.0.
- Physical Form: Supplied as a translucent liquid or paste with a slight odor.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Appearance
Translucent
Chemistry Type
Silicone
Physical Properties
Extrusion Rate
150 to 500 g/min
Mechanical Properties
Elongation
115 %
Chemical Properties
Water Absorption
1.4 %
Other Properties
Storage Temperature
8 °C - 28 °C