LOCTITE M2013RS
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other
Main features
- One-Component Screen Printing
- 2-Minute 200 deg C Drying
- 1% Laser-Trimming Linearity
Product Description
LOCTITE M2013RS is a one-component conductive ink supplied in a 1 kg container for screen-printing printed-electronics features. Compatible substrates include FR-3, FR-4, CEM-1, CEM-3, polyester sulfone, and ceramic. Its optimum drying cycle is 2 minutes at 200 deg C, followed by heat or infrared cure. It is laser trimmable with 1% linearity and has high wear resistance. The one-component format combines screen-printing application with a defined thermal drying and cure sequence for conductive printed features.
Key features
- Screen-Printable One-Component Ink: The format supports screen printing of conductive printed-electronics features.
- Thermal Drying Cycle: Optimum drying is 2 minutes at 200 deg C.
- Laser-Trim Control: Laser-trimming linearity is 1%.
Applications
Compatible substrates include FR-3, FR-4, CEM-1, CEM-3, polyester sulfone, and ceramic.