LOCTITE M2013-5RS

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

LOCTITE M2013-5RS

Main features

  • 2-Minute 200 deg C Drying
  • 1% Laser-Trimming Linearity
  • Heat- and IR-Cure Processing

Product Description

LOCTITE M2013-5RS E&C is a one-component screen-printable conductive ink supplied in a 1 kg container for printed-electronics processing. The optimum drying cycle is 2 minutes at 200 deg C, with heat or infrared cure. It is laser trimmable with 1% linearity. Compatible substrates include FR-3, FR-4, CEM-1, CEM-3, polyester sulfone, and ceramic. The screen-printable, one-component format supports low-profile conductive features on the listed substrates during printed-electronics production, heat curing, infrared curing, and laser trimming.

Key features

  • Thermal Drying Cycle: Optimum drying is 2 minutes at 200 deg C.
  • Laser-Trim Control: Laser-trimming linearity is 1%.
  • Heat and IR Cure: The one-component conductive ink can be processed by heat or infrared cure.

Applications

Compatible substrates include FR-3, FR-4, CEM-1, CEM-3, polyester sulfone, and ceramic.

Product Family

LOCTITE M2013-5RS

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Thermal Properties
Flash Point
115.6 °C
Physical Properties
Viscosity
28,000 - 32,000 mPa.s
VOC
403.00 g/L