LOCTITE LB 8213
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- 0.362 mm Four-Ball Wear Scar
- -26 to 260 deg C Operating Range
- PFPE/PTFE NLGI 2 Grease
Product Description
LOCTITE LB 8213 is a one-component, non-curing synthetic grease with PFPE base oil and a PTFE thickener. It lubricates bearings and valves in equipment such as conveyor bearings, high-temperature fans, motors, textile machinery, and ventilation systems. Typical application operating range is -26 to 260 deg C. The base oil viscosity is 810 cSt at 20 deg C by ASTM D445, and the grease is NLGI Class 2. ASTM D2266 data include a 0.362 mm four-ball wear scar and a coefficient of friction of 0.11.
Key features
- PFPE/PTFE NLGI 2 Grease: PFPE base oil with PTFE thickener in a non-curing synthetic grease.
- 0.362 mm Wear Scar: Four-ball wear scar is 0.362 mm by ASTM D2266.
- -26 to 260 deg C Range: Typical application operating range is -26 to 260 deg C.
Applications
Bearings and valves in conveyors, fans, motors, textile equipment, welding machines, and other high-temperature machinery.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Other Properties
Additional Information
As supplied
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Base oil | PFPE | As supplied | |
| Thickener | PTFE | As supplied | |
| Specific gravity | 1.95 | 25 deg C | |
| Base-oil viscosity | 810 | cSt | ASTM D445, 20 deg C |
| NLGI class | 2 | ISO 6743-99 | |
| Penetration | 265 to 290 | 1/10 mm | ISO 2137 |
In service
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Operating range | -26 to 260 | deg C | Typical application range |
| Oil separation | 3.0 | % wt. loss | ASTM D6184, 30 h at 99 deg C |
| Four-ball wear scar | 0.362 | mm | ASTM D2266 |
| Coefficient of friction | 0.11 | ASTM D2266 |