LOCTITE LB 8013

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE LB8013

Main features

  • Metal-Free High-Purity Anti-Seize
  • Calcium Oxide/Graphite Lubrication
  • High-Temperature Thread Protection

Product Description

LOCTITE LB 8013 is a non-curing, high-purity metal-free anti-seize lubricant based on calcium oxide and graphite. The dark gray one-component paste is made from high-purity raw materials with trace limits for halogens, sulfur, copper, aluminum, and heavy metals. Its operating range is -29 to 1315 deg C, and LMS contaminant limits include chloride at most 50 ppm, sulfur at most 100 ppm, and copper at most 50 ppm. The lubricant is used on steel, stainless steel, and selected alloy assemblies to reduce high friction, galling, and seizing during assembly and disassembly. Applications include bolts, valves, studs, pipe fittings, slip fits, and press fits.

Key features

  • Metal-Free High-Purity Formula: Calcium oxide/graphite anti-seize made from high-purity raw materials with controlled trace contaminants.
  • High-Temperature Operating Range: Used across an operating range of -29 to 1315 deg C.
  • Torque and Galling Control: Used on steel and stainless-steel assemblies to reduce friction, galling, and seizing.

Applications

Bolts, valves, studs, pipe fittings, slip fits, and press fits in high-temperature industrial anti-seize service.

Technical Specifications

General Properties
Appearance
Dark gray paste
Chemistry Type
Calcium Oxide/Graphite Based
Specific Gravity
1.12 to 1.27
Other Properties
Storage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Specific gravity1.12 to 1.27-LMS range; 25 deg C
Penetration, unworked320 to 3801/10 mmLMS range; ISO 2137
Operating range-29 to 1315deg CTypical application range
Chloride<=50ppmLMS maximum ionic contaminant
Sulfur<=100ppmLMS maximum ionic contaminant
Copper<=50ppmLMS maximum ionic contaminant

Leading Brands Trust in Our Products and Services