LOCTITE LB 8007

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE LB8007

Main features

  • Copper/Graphite Anti-Seize Protection
  • High-Temperature Threaded Assembly Service
  • Lower-Friction Threaded Assembly

Product Description

LOCTITE LB 8007 is a non-curing copper/graphite anti-seize lubricant for threaded and assembled components exposed to heat, seizing, and galling. The smooth copper-colored paste has 40% nonvolatile content, a typical density of 1.27 g/mL at 25 deg C, and an operating range of -29 to 982 deg C. It is applied as a thin coating to threads and flats before assembly. In the specified 12.7 mm grade 8 steel bolt and grade 5 nut test, the lubricated torque coefficient is 0.16 compared with 0.27 for solvent-cleaned unlubricated fasteners. Applications include screws, nuts, pipes, exhaust hardware, brake bolts, studs, flanges, and gaskets.

Key features

  • Copper/Graphite Anti-Seize: Smooth copper-colored anti-seize paste for threaded and assembled components.
  • High-Temperature Assembly Range: Used across an operating range of -29 to 982 deg C.
  • Lower Thread Friction: For 12.7 mm grade 8 steel bolts and grade 5 nuts, torque coefficient is 0.16 lubricated versus 0.27 solvent-cleaned and unlubricated.

Applications

Screws, nuts, pipes, exhaust and brake bolts, studs, flanges, and gaskets.

Technical Specifications

General Properties
Appearance
Smooth copper colored paste
Density (g)
1.27 g/cm3
Solids
40 %
Specific Gravity
1.2 to 1.4
Other Properties
Storage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Specific gravity1.2 to 1.4-LMS range; 25 deg C
Density1.27g/mLTypical; 25 deg C
Solids / nonvolatile content40%Typical
Penetration320 to 3801/10 mmLMS range; ISO 2137
Operating range-29 to 982deg CTypical application range