LOCTITE EDAG 440
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other
Main features
- High Electrical Conductivity
- High Coverage Efficiency
- Room-Temperature Cure
Product Description
LOCTITE EDAG 440 AS E&C is a nickel-filled thermoplastic conductive coating designed for electromagnetic compatibility (EMC) shielding in electronic equipment housings. The coating provides high electrical conductivity for EMI shielding and electrostatic discharge (ESD) protection while offering high coverage, over-coatability, and improved sedimentation stability. It cures at room temperature and can be applied by spray coating to plastic housings and antenna components. Typical applications include reflective coatings on parabolic antennas and EMC shielding for consumer electronics and medical equipment enclosures.
Key features
- High electrical conductivity: Supports EMI shielding and ESD protection in electronic enclosure applications.
- High coverage efficiency: Delivers theoretical coverage of approximately 17 m²/kg at 10 µm coating thickness.
- Room-temperature cure: Dries rapidly and can also be force-dried for accelerated production processing.
Applications / Suitable for
- EMC shielding coatings for electronic equipment housings
- Consumer electronics plastic enclosures
- Medical equipment housings
- Reflective coatings on parabolic antennas
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied characteristics of LOCTITE EDAG 440 AS E&C.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Nickel | — | As supplied |
| Solids Content | 68 | % | Typical value |
| Viscosity | 5,750 | mPa·s (cP) | 20°C, 20 rpm |
| Density | 2,025 | kg/m³ | Typical value |
| Theoretical Coverage | 17 | m²/kg | At 10 µm coating thickness |
| Shelf Life | 1 | Year | Stored at 5–30°C |
After-processing / final-state properties
Typical properties measured on Lexan panels after overnight air drying.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Attenuation | 50–70 | dB | 50 µm coating thickness |
| Adhesion | 5B | — | Lexan panels, air dried overnight |
| Pencil Hardness | 9H | — | Lexan panels, air dried overnight |
| Sheet Resistivity | <0.5 | ohm/sq | 1 mil coating thickness |
| Operating Temperature | -40 to 95 | °C | Typical operating range |