Loctite EA 9360 AERO Epoxy Adhesive

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite EA 9360 AERO Epoxy Adhesive

Main features

  • Toughened Structural Epoxy Bonding
  • 50-Minute Assembly Pot Life
  • Room-Temperature Aircraft Bonding Cure

Product Description

LOCTITE® EA 9360 AERO is a two-component, toughened epoxy paste adhesive that cures at room temperature and combines high room-temperature peel strength with tensile lap shear performance at elevated temperatures. Its low-slump consistency supports controlled application, while the 50-minute pot life at 77°F (25°C), 200 g mass, provides time for mixing and assembly. The adhesive develops handling strength after 24 hours at 77°F (25°C) and reaches normal performance after a 5–7 day room-temperature cure. Accelerated curing may be used for small masses, including 1 hour at 180°F (82°C). It is also available in dual-cartridge packaging for two-component dispensing.

Key features

  • High peel strength: Delivers a typical floating-roller peel strength of 68 lb/in (303 N/25 mm) after 7 days at 77°F (25°C) on prepared and primed 2024-T3 AlClad aluminum.
  • Elevated-temperature bond performance: Retains typical tensile lap shear strength of 2,000 psi (13.8 MPa) at 225°F (107°C) on phosphoric-acid-anodized 2024-T3 bare aluminum.
  • Room-temperature or accelerated cure: Reaches normal performance after 5–7 days at 77°F (25°C), with accelerated cures up to 200°F (93°C) available for small adhesive masses.

Technical Specifications

General Properties
Component System
Two Part (A/B)
Mechanical Properties
Elongation
5 %
Thermal Properties
Thermal Conductivity
0.25 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured, mixing, working-time, storage and cure information for LOCTITE® EA 9360 AERO. Component and mixed-material values are identified separately.

Property Value Unit Method / condition
Product type Two-component toughened epoxy paste adhesive — Requires mixing before application
Color — Part A Off-white — Unmixed component
Color — Part B Blue — Unmixed component
Viscosity — Part A 3,000 Poise 77°F; Brookfield HBT, spindle 7 at 20 rpm
Viscosity — Part B 1,700 Poise 77°F; Brookfield HBT, spindle 6 at 20 rpm
Viscosity — Mixed 1,200 Poise 77°F; Brookfield HBT, spindle 5 at 20 rpm
Viscosity — Part A 300 Pa·s 25°C; Brookfield HBT at 2.1 rad/s
Viscosity — Part B 170 Pa·s 25°C; Brookfield HBT at 2.1 rad/s
Viscosity — Mixed 120 Pa·s 25°C; Brookfield HBT at 2.1 rad/s
Density — Part A 1.16 g/mL Unmixed component
Density — Part B 1.00 g/mL Unmixed component
Density — Mixed 1.14 g/mL Mixed adhesive
Mix ratio by weight — Part A:Part B 100:43 Parts by weight Components must be mixed thoroughly
Mix ratio by volume — Part A:Part B 2:1 Parts by volume Volume measurement is not recommended for structural applications unless precautions ensure the correct ratio
Pot life 50 minutes 200 g mass at 77°F (25°C); ASTM D2471, water bath
Maximum recommended mixed quantity 450 g Do not mix larger quantities because hazardous heat buildup and uncontrolled decomposition may occur
Handling strength 24 hours At 77°F (25°C); full bond strength has not yet developed
Room-temperature cure 5–7 days At 77°F (25°C) to achieve normal performance
Example accelerated cure 1 hour at 180°F (82°C) — Complete cure; accelerated cures up to 200°F (93°C) are for small masses only
Shelf life — Part A and Part B 1 year Stored below 40°F (4°C)
Shelf life — Part A and Part B 6 months Stored below 77°F (25°C)
Shelf life — Part A and Part B 6 months Stored below 90°F (32°C)