LOCTITE EA 9203
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other
Main features
- No-Bake Room-Temperature Priming
- Brush-or-Spray Application Flexibility
- Adhesion Promotion on Limited-Preparation Surfaces
Product Description
LOCTITE EA 9203 AERO is a one-component, non-curing aerospace adhesive-bonding primer used to enhance adhesion on poorly prepared surfaces. It is supplied as a blue primer and may be applied by brush or spray. The material is used as received after warming to room temperature and thorough mixing. Applied surfaces air dry at room temperature and do not require baking or chemical cure; allow at least 1 hour of air drying before bonding. Spray application targets a dry primer film thinner than 0.003 mm. The primer is especially suited to room-temperature-curing paste adhesives.
Key features
- No-Bake Air Drying: The non-curing primer air dries at room temperature and does not require baking.
- Brush or Spray Application: Apply the one-component primer after warming to room temperature and thorough mixing.
- Adhesion on Poorly Prepared Surfaces: The primer enhances adhesion and is especially suited to room-temperature-curing paste adhesives.
Applications
Aerospace adhesive bonding, including use with room-temperature-curing paste adhesives and surfaces with limited preparation.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Blue | As supplied | |
| Density | 0.8 | g/ml | As supplied |
| Shelf life | 1 | year | Stored at 25 deg C |