LOCTITE® AA 312™ is a one-component modified acrylic ester adhesive formulated for bonding dissimilar materials, including metals, glass, and ceramics. Used with LOCTITE® Activator 736™ or 734™, the adhesive cures at room temperature and provides rapid fixture times for close-fitting assemblies. Its medium-viscosity formulation requires no mixing, making it suitable for manufacturing and industrial bonding applications where fast processing and reliable bond development are required.

Key features

  • One-component formulation: Requires no mixing, simplifying application and assembly processes.
  • Room-temperature cure: Cures with LOCTITE® Activator 736™ or 734™ to support rapid fixture times.
  • Dissimilar material bonding: Suitable for bonding metals, glass, and ceramics in close-fitting assemblies.

Applications / Suitable for

  • Metal-to-metal bonding
  • Glass bonding applications
  • Ceramic assembly applications
  • Industrial manufacturing and assembly operations
  • Close-fitting bonded joints requiring fast fixturing

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of LOCTITE® AA 312™ before curing and assembly.

Property Value Unit Method / condition
Chemical Type Modified acrylic ester - As supplied
Appearance Clear amber liquid - Uncured material
Specific Gravity 1.1 - 25°C
Viscosity 850-1,200 mPa·s (cP) Brookfield RVT, Spindle 2, 20 rpm, 25°C
Technical properties

After-processing / final-state properties

Typical cured-material properties and lap shear strength performance data.

Property Value Unit Method / condition
Coefficient of Thermal Expansion 100 × 10⁻⁶ K⁻¹ ISO 11359-2
Thermal Conductivity 0.1 W/(m·K) ISO 8302
Specific Heat 0.3 kJ/(kg·K) Cured material
Lap Shear Strength ≥17.2 N/mm² ISO 4587, steel (grit blasted), 24 h @ 22°C, Activator 736™ or 734™ on 2 sides