LAIRD TFLEX P130

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD TFLEX P130

Main features

  • Shore 00 13 Conformability
  • Integrated Tgard Handling Liner
  • 30 Mil Controlled Thickness

Product Description

Tflex P130 is a 0.030 in (0.75 mm) soft silicone thermal gap filler with an integrated Tgard liner. The yellow elastomer provides 1.2 W/(m K) thermal conductivity and Shore 00 hardness of 13, helping it conform around component height variation at low assembly pressure. Its liner supports handling and placement of the preformed sheet while preserving a controlled nominal thickness. The material operates from -40 to 200 deg C and includes dielectric, volume-resistivity, and breakdown-voltage data for electrical-isolation screening. It is intended for compact electronics interfaces that need soft compliance, reinforced handling, and repeatable pad placement.

Key features

  • Soft gap conformity: Shore 00 hardness of 13 supports low-pressure compression.
  • Integrated Tgard liner: Reinforced construction supports handling and placement.
  • 30 mil nominal thickness: Preformed 0.030 in sheet supports controlled gap filling.

Applications

Automotive ADAS; Automotive Electronics; Automotive Infotainment; Automotive Powertrain/ECUs; Drones/Satellites; Gaming Systems; Instrumentation; Notebooks/Tablets/Portable Devices; Routers; Smart Home Devices; Wireless infrastructure

Technical Specifications

General Properties
Color
Yellow
Density (g)
2.3 g/cm3
Thermal Properties
Temperature Range
-40°C to 200 °C
Thermal Conductivity
1.2 W/m.K
Electrical Properties
Volume Resistivity
1.3×10¹² Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ConstructionTgard-lined silicone elastomerLaird Tflex P100 datasheet
Nominal thickness0.75 (0.030)mm (in)Exact Tflex P130 part page
ColorYellowVisual
Density2.30g/ccHelium pycnometer
Hardness13Shore 00ASTM D2240
Shelf life2yearsFrom date of shipment
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Thermal conductivity1.20W/(m K)ASTM D5470
Operating temperature range-40 to 200deg CLaird test
Dielectric constant7.501 MHz; ASTM D150
Volume resistivity1.2 x 10^13ohm-cmASTM D257
Breakdown voltage> 9kVASTM D149