LAIRD TFLEX HD91500

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD TFLEX HD91500

Main features

  • High-Conductivity Gap Bridging
  • Low-Pressure Surface Conformance
  • 1500-um Thickness Availability

Product Description

Tflex HD91500 provides the Tflex HD90000 high-deflection material in a 9 x 9 in sheet at a nominal 1500 um (0.060 in) thickness. Its grey ceramic-filled silicone construction combines 7.5 W/(m K) thermal conductivity with low pressure-versus-deflection performance. Surface wetting reduces contact resistance and mechanical stress at the interface. The material has Shore 00 hardness of 32 for thicknesses of 1000 um and above, plus 0.17% TML and 0.01% CVCM outgassing values by ASTM E595. The 60 mil grade applies to automotive electronics, drones and satellites, instrumentation, portable devices, routers, and smart-home equipment.

Key features

  • 1500 um thermal sheet: Supplies a nominal 0.060 in grade in a 9 x 9 in format.
  • High-deflection interface: Conforms at low pressure to reduce component stress.
  • Controlled outgassing: Combines low TML and CVCM values with 7.5 W/(m K) conductivity.

Applications

Automotive ADAS; automotive electronics; automotive infotainment; automotive powertrain/ECUs; drones and satellites; gaming systems; instrumentation; notebooks, tablets, and portable devices; routers; smart-home devices; wireless infrastructure.

Technical Specifications

General Properties
Color
Grey
Density (g)
3.5 g/cm3
Thermal Properties
Operating Temperature
-65°C to 125 °C
Thermal Conductivity
7.5 W/m.K
Electrical Properties
Volume Resistivity
8.73×10¹³ Ohms⋅cm

Additional Information

Technical properties

As-Supplied Properties

Grade-specific nominal thickness and sheet size; remaining values are typical for the Tflex HD90000 material family.

PropertyValueUnitMethod / condition
Nominal thickness1500umPart-number convention; 0.060 in
Thickness tolerance+/- 10%Nominal
Construction and compositionCeramic-filled silicone sheetComposition
ColorGreyVisual
Density3.5g/cm^3Helium pycnometer
Hardness32Shore 00ASTM D2240
Sheet size9 x 9inExact grade format
Technical properties

Installed Interface Properties

Typical Tflex HD90000 material-family properties; thermal resistance is measured at 40 mil, 10 psi, and 50 deg C.

PropertyValueUnitMethod / condition
Thermal conductivity7.5W/(m K)Hot Disk
Thermal resistance0.198deg C in^2/WASTM D5470; 40 mil, 10 psi, 50 deg C
Temperature range-65 to 125deg CLaird test method
Dielectric constant8.14ASTM D150; 1 MHz
Volume resistivity8.73 x 10^13ohm-cmASTM D257
UL flammability ratingV-0UL 94