LAIRD TFLEX HD740

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD TFLEX HD740

Main features

  • Surface-Wetting Contact Performance
  • Low-Resistance Thermal Interface
  • 0.040-Inch Thickness Selection

Product Description

Tflex HD740 brings the 5.0 W/(m K) Tflex HD700 material to a nominal 0.040 in thermal gap-filler sheet. Its high-deflection silicone construction wets interface surfaces and compresses with low pressure, reducing contact resistance and component stress while maintaining the conductive thermal path. The pink sheet has a +/-10% thickness tolerance, a 3.3 g/cm^3 density, Shore 00 hardness of 54, and a -50 to 200 deg C temperature range. The 40 mil grade is relevant to automotive electronics, drones and satellites, gaming systems, instrumentation, portable devices, routers, and smart-home equipment.

Key features

  • 40 mil interface grade: Provides a nominal 0.040 in thermal gap-filler thickness.
  • Surface-wetting contact: Reduces contact resistance across mating surfaces.
  • Low-pressure heat transfer: Combines compliant deflection with 5.0 W/(m K) conductivity.

Applications

Automotive ADAS; automotive electronics; automotive infotainment; automotive powertrain/ECUs; drones and satellites; gaming systems; instrumentation; notebooks, tablets, and portable devices; routers; smart-home devices; wireless infrastructure.

Technical Specifications

General Properties
Color
Pink
Density (g)
3.3 g/cm3
Thermal Properties
Temperature Range
-50°C to 200 °C
Thermal Conductivity
2.7 W/m.K
Electrical Properties
Volume Resistivity
1.4x10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-Supplied Properties

Grade-specific nominal thickness; remaining values are typical for the Tflex HD700 material family.

PropertyValueUnitMethod / condition
Nominal thickness0.040inPart-number convention
Thickness tolerance+/- 10%Nominal
Construction and compositionCeramic-filled silicone sheetComposition
ColorPinkVisual
Density3.3g/cm^3Helium pycnometer
Hardness54Shore 00ASTM D2240
Technical properties

Installed Interface Properties

Typical Tflex HD700 material-family properties; thermal resistance is measured at 40 mil and 10 psi.

PropertyValueUnitMethod / condition
Thermal conductivity5.0W/(m K)ASTM D5470
Thermal resistance0.287deg C in^2/WASTM D5470 (modified); 40 mil, 10 psi
Temperature range-50 to 200deg CLaird test method
Dielectric constant5.01ASTM D150; 1 MHz
Volume resistivity1.4 x 10^14ohm-cmASTM D257
UL flammability ratingV-0UL 94