LAIRD TFLEX HD380

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD TFLEX HD380

Main features

  • 80-Mil Variable-Gap Coverage
  • Low-Resistance Surface Wetting
  • Low-Stress Board Interface

Product Description

Tflex HD380 provides the Tflex HD300 high-deflection gap-filler material in a nominal 0.080 in sheet. The pink ceramic-filled silicone construction offers 2.7 W/(m K) thermal conductivity and conforms across manufacturing tolerances with low pressure-versus-deflection behavior. Strong surface wetting reduces contact resistance while the compliant pad limits mechanical loading on boards and components. Typical family properties include 3.1 g/cm^3 density, Shore 00 hardness of 38, and a -40 to 200 deg C temperature range. The 80 mil grade fits thermal-management assemblies in automotive electronics, gaming systems, instrumentation, portable devices, routers, and wireless infrastructure.

Key features

  • 80 mil thickness: Provides the Tflex HD300 material at a nominal 0.080 in.
  • High-deflection interface: Fills manufacturing-tolerance gaps with low mechanical loading.
  • Low contact resistance: Surface wetting complements 2.7 W/(m K) thermal conductivity.

Applications

Automotive ADAS; automotive electronics; automotive infotainment; automotive powertrain/ECUs; drones and satellites; gaming systems; instrumentation; notebooks, tablets, and portable devices; routers; smart-home devices; wireless infrastructure.

Technical Specifications

General Properties
Color
Pink
Density (g)
3.1 g/cm3
Thermal Properties
Operating Temperature
-40°C to 200 °C
Thermal Conductivity
2.7 W/m.K
Electrical Properties
Volume Resistivity
1.2x10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-Supplied Properties

Grade-specific nominal thickness; remaining values are typical for the Tflex HD300 material family.

PropertyValueUnitMethod / condition
Nominal thickness0.080inPart-number convention
Thickness tolerance+/- 10%Nominal
Construction and compositionCeramic-filled silicone sheetComposition
ColorPinkVisual
Density3.1g/cm^3Helium pycnometer
Hardness38Shore 00ASTM D2240
Technical properties

Installed Interface Properties

Typical Tflex HD300 material-family properties; thermal resistance is measured at 40 mil and 10 psi.

PropertyValueUnitMethod / condition
Thermal conductivity2.7W/(m K)ASTM D5470
Thermal resistance0.573deg C in^2/WASTM D5470 (modified); 40 mil, 10 psi
Temperature range-40 to 200deg CLaird test method
Dielectric constant6.62ASTM D150; 1 MHz
Volume resistivity1.2 x 10^14ohm-cmASTM D257
UL flammability ratingV-0UL 94