LAIRD TFLEX HD350

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD TFLEX HD350

Main features

  • 0.050-Inch Variable-Gap Interface
  • 2.7 W/(m K) Interface Heat Transfer
  • Low-Pressure High-Deflection Conformance

Product Description

Tflex HD350 combines a 0.050 in (1.25 mm) nominal thickness with the high-deflection construction of the Tflex HD300 silicone thermal gap-filler family. Typical 2.7 W/(m K) thermal conductivity and surface wetting support a low-resistance thermal interface. Low pressure-versus-deflection characteristics accommodate manufacturing tolerances while limiting board and component stress. The pink, naturally tacky pad has typical Shore 00 hardness of 38, a +/- 10% thickness tolerance, and an operating range of -40 to 200 deg C. A removable liner protects the placement surface before assembly.

Key features

  • 50-mil gap pad: 0.050 in (1.25 mm) preformed interface.
  • Thermal conductivity: Typical 2.7 W/(m K) conductivity supports interface heat transfer.
  • Low-pressure deflection: High-deflection construction accommodates variable gaps with limited component stress.

Applications

Applications include automotive electronics, drones and satellites, instrumentation, routers, and notebooks, tablets, and other portable devices.

Technical Specifications

General Properties
Color
Pink
Density (g)
3.1 g/cm3
Thermal Properties
Operating Temperature
-40°C to 200 °C
Thermal Conductivity
2.7 W/m.K
Electrical Properties
Volume Resistivity
1.2x10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-supplied properties

Typical Tflex HD300 family data for the Tflex HD350 thickness grade.

PropertyValueUnitMethod / condition
ConstructionCeramic-filled silicone sheet-Typical family construction
Nominal thickness0.050 (1.25)in (mm)Tflex HD350 grade
Thickness tolerance+/- 10%Typical family tolerance
ColorPink-Visual
Density3.1g/cm^3Typical; helium pycnometer
Hardness38Shore 00Typical; ASTM D2240
Shelf life2yearsFrom shipment; store at 0 to 35 deg C in original packaging
Technical properties

Installed / in-service properties

Typical Tflex HD300 family data for the Tflex HD350 thickness grade.

PropertyValueUnitMethod / condition
Thermal conductivity2.7W/(m K)Typical; ASTM D5470
Temperature range-40 to 200deg CLaird test method
Dielectric constant6.62-Typical; 1 MHz, ASTM D150
Volume resistivity1.2 x 10^14ohm cmTypical; ASTM D257
Flammability ratingV-0-UL 94

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers