LAIRD TFLEX 7200

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD TFLEX 7200

Main features

  • 0.200-Inch Preformed Gap Control
  • Compliant Low-Pressure Heat Transfer
  • Electrically Insulating Gap Pad

Product Description

Tflex 7200 is the 0.200 in (5.08 mm) thickness grade of the silicone Tflex 700 thermal gap-filler family. This preformed dark gray sheet has typical 5.0 W/(m K) thermal conductivity and a highly compliant construction for contact with uneven component topography. Low thermal resistance at low pressure and natural tack support placement between electronic components and mating chassis or parts. The material is electrically insulating, carries a UL 94 V-0 flammability rating, and operates from -40 to 200 deg C.

Key features

  • 200-mil sheet: 0.200 in (5.08 mm) nominal gap-filler thickness.
  • Low-pressure interface: High compliancy maintains low thermal resistance at low pressure.
  • Electrical insulation: Typical dielectric constant is 7.80 with 1.00 x 10^13 ohm cm volume resistivity.

Applications

Applications include automotive powertrain and ECUs, gaming systems, smart home devices, drones and satellites, and wireless infrastructure.

Product Family

LAIRD TFLEX 7200

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Dark Grey
Specific Gravity
1.73
Thermal Properties
Operating Temperature
-40°C to 200 °C
Thermal Conductivity
5.0 W/m.K

Additional Information

Technical properties

As-supplied properties

Typical Tflex 700 family data for the Tflex 7200 thickness grade.

PropertyValueUnitMethod / condition
ConstructionFilled silicone sheet-Typical family construction
Nominal thickness0.200 (5.08)in (mm)Tflex 7200 grade
ColorDark gray-Visual
Density1.70g/cm^3Typical
Shelf life2yearsFrom date of shipment
Technical properties

Installed / in-service properties

Typical Tflex 700 family data for the Tflex 7200 thickness grade.

PropertyValueUnitMethod / condition
Thermal conductivity5.0W/(m K)Typical; Hot Disk
Operating temperature-40 to 200deg CRange
Dielectric constant7.80-Typical
Volume resistivity1.00 x 10^13ohm cmTypical
Flammability ratingV-0-UL 94

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers