LAIRD TFLEX 6200

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD TFLEX 6200

Main features

  • Maximum 0.200-Inch Standard Format
  • 3.0 W/(m K) Thermal Transfer
  • Compliant Adhesive-Free Interface Placement

Product Description

Tflex 6200 is the nominal 0.200 in Tflex 600 grade and the thickest standard family format identified by the part-number system. This ceramic-filled silicone gap-filler sheet combines typical 3.0 W/(m K) thermal conductivity with highly compliant, low-stress interface contact. The naturally tacky material needs no further adhesive coating and is electrically insulating. Typical volume resistivity is 2 x 10^13 ohm cm, and the family temperature range is -45 to 200 deg C. Applications include automotive electronics, drones and satellites, gaming systems, instrumentation, portable devices, routers, smart-home devices, and wireless infrastructure.

Key features

  • Maximum standard thickness: The nominal 0.200 in format is the upper end of the standard Tflex 600 thickness range.
  • 3.0 W/(m K) conductivity: Typical thermal conductivity is measured by ASTM D5470.
  • Compliant tacky interface: High compliance and natural tack support low-stress placement without added adhesive coating.

Applications

Automotive ADAS; automotive electronics; drones and satellites; gaming systems; instrumentation; notebooks, tablets, and portable devices; wireless infrastructure.

Technical Specifications

General Properties
Color
Blue-Violet
Density (g)
1.34 g/cm3
Thermal Properties
Temperature Range
-45°C to 200 °C
Thermal Conductivity
3.0 W/m.K
Electrical Properties
Volume Resistivity
2x10¹³ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Tflex 6200 is the nominal 0.200 in Tflex 600 grade; other values are typical for Tflex 600 material.

PropertyValueUnitMethod / condition
Construction and compositionCeramic-filled silicone sheet-As supplied
ColorBlue-violet-Visual; typical
Nominal thickness0.200inGrade code; thickness in mils
Hardness51Shore 00ASTM D2240; typical
Surface tackNaturally tacky on both sides-Standard construction; DC option changes tack configuration
ReinforcementNot required-Thicknesses of 0.040 in and above
Technical properties

After-processing / final-state properties

Typical Tflex 600 material data; thermal conductivity is a bulk value, not complete installed-interface performance.

PropertyValueUnitMethod / condition
Thermal conductivity3.0W/(m K)ASTM D5470; typical
Temperature range-45 to 200deg CTypical
Volume resistivity2 x 10^13ohm cmASTM D257; typical
Outgassing TML0.65%ASTM E595; typical
Outgassing CVCM0.21%ASTM E595; typical