LAIRD TFLEX 3140

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD TFLEX 3140

Main features

  • 3.56 mm Gap-Filling Thickness
  • High-Compliancy Interface Contact
  • Reusable Low-Compression-Set Pad

Product Description

Tflex 3140 is a 3.56 mm preformed silicone thermal gap-filler sheet for filling interface gaps around electronic components. The ceramic-filled material has typical thermal conductivity of 1.2 W/(m K) and deflects more than 50% of its original thickness at 50 psi. With Shore 00 hardness of 25.2 for 40 mil and thicker material, it conforms under pressure while retaining the low-compression-set behavior of the Tflex 300 series. The light-green sheet operates from -40 to 160 deg C.

Key features

  • Preformed 3.56 mm sheet: Supplies the exact thickness assigned to the 3140 grade.
  • High compliance: Deflects more than 50% of its original thickness at 50 psi.
  • Thermal conductivity: Typical conductivity is 1.2 W/(m K) by ASTM D5470.

Applications

Applications include automotive ADAS and electronics, gaming systems, instrumentation, portable devices, routers and wireless infrastructure.

Technical Specifications

General Properties
Color
Light Green
Density (g)
1.80 g/cm3
Length
457 mm
Width
45.7 cm
Thermal Properties
Operating Temperature
-40 to 160 °C
Thermal Conductivity
1.20 W/m.K
Electrical Properties
Volume Resistivity
1.00 x10^13 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Values describe the supplied preformed sheet before installation.

PropertyValueUnitMethod / condition
Construction and compositionCeramic-filled silicone sheetTypical
ColorLight greenVisual
Nominal thickness3.56mmExact grade
Density1.78g/cm^3Helium pycnometer
Hardness25.2Shore 0040 mil and thicker; ASTM D2240
Shelf life2yearsFrom date of shipment
Technical properties

After-processing / final-state properties

Values describe bulk or compressed material under the stated test conditions, not complete assembly performance.

PropertyValueUnitMethod / condition
DeflectionMore than 50%At 50 psi; relative to original thickness
Thermal conductivity1.2W/(m K)ASTM D5470; typical
Operating temperature-40 to 160deg CTypical range
Dielectric constant4.5At 10 GHz; ASTM D150
Volume resistivity10^13ohm cmASTM D257