LAIRD SF4.5

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LAIRD SF4.5

Main features

  • 4.5 GHz Narrow-Band Absorption
  • Flexible Metal-Surface Conformability
  • 163 deg C Service Capability

Product Description

Eccosorb SF-4.5 is a black, silicone-based free-space resonant absorber sheet for narrow-band microwave reflection control at a 4.5 GHz design frequency. The 305 x 305 mm sheet is 2.30 mm thick and can be bonded to flat or curved metallic surfaces. Its flexible construction combines 73 Shore A hardness with a maximum service temperature of 163 deg C. The material addresses reflections, echoes, surface currents and cavity resonances in microwave assemblies. It is supplied as a free-space elastomer for metallic microwave structures.

Key features

  • 4.5 GHz resonant response: Targets narrow-band free-space absorption at the exact design frequency.
  • Flexible silicone sheet: Bonds to flat or curved metallic surfaces for reflection control.
  • Maximum service temperature: Operates to a maximum of 163 deg C.

Applications

Applications include avionics; base stations, power amplifiers, active antenna units and small cells; naval and maritime systems; radar; and satellites.

Product Family

LAIRD SF4.5

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Resin: Silicone
Color
Black
Density (g)
2.40 g/cm3
Functionality
Free Space
Thermal Properties
Operating Temperature
163 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Values describe the supplied silicone elastomer absorber sheet.

PropertyValueUnitMethod / condition
ColorBlackTypical
Density3.90g/cm^3Typical
Nominal thickness2.30mmExact part
Sheet dimensions305 x 305mmExact part
Hardness73Shore ATypical
Shelf lifeMinimum 720daysFrom date of shipment
Technical properties

After-processing / final-state properties

Mechanical and power-handling values are typical for the Eccosorb SF family.

PropertyValueUnitMethod / condition
Design frequency4.5GHzExact part
Maximum service temperature163deg CTypical
Power handling0.2W/cm^2Typical
Tensile strength1.0 to 6.0MPaTypical family range
Elongation at break20 to 100%Typical family range
Tear strength0.2 to 2.0N/mmTypical family range