LAIRD NS1000C
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- 110 Initial Permeability at 1 MHz
- 20-MHz-to-3-GHz Noise Suppression
- Thin Flexible PSA-Optional Formats
Product Description
NoiseSorb NS1000C is the 110 initial-permeability sub-series within Laird's ultrathin NS1000 near-field EMI absorber family. At 1 MHz, its typical initial permeability is 110, with a family effective range of 20 MHz to 3 GHz for suppressing unwanted coupling, radiated noise, resonances, and surface currents. The flexible absorber is available in 0.05 to 0.5 mm thicknesses with or without pressure-sensitive adhesive and operates from -40 to 105 deg C. NS1000C can be placed over processors, memory devices, power ICs, flat cables, high-speed transmission lines, displays, and other circuit-board elements in automotive, medical, networking, computing, and telecommunications equipment.
Key features
- 110 initial permeability: NS1000C has typical initial permeability of 110 at 1 MHz.
- Broad near-field suppression: The effective frequency range is 20 MHz to 3 GHz.
- Thin configurable sheets: Thicknesses from 0.05 to 0.5 mm are available with or without PSA.
Applications
Near-field EMI suppression around processors, memory, power ICs, cables, high-speed traces, displays, and circuit-board elements.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Typical NS1000C sub-series design data for product selection; values are not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Family position | NS1000C sub-series | Within NS1000 parent family | |
| Initial permeability | 110 | 1 MHz; typical | |
| Effective frequency range | 20 MHz to 3 GHz | Typical | |
| Surface resistivity | Above 1 x 10^6 | ohm/sq | Typical |
| Thermal conductivity | 1.0 | W/mK | Typical |
| Operating temperature | -40 to 105 | deg C | Typical |
| Available thickness | 0.05 to 0.5 | mm | Sub-series range |
| Backing | With or without PSA | Available configuration |