LAIRD A10095-02

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LAIRD A10095-02

Main features

  • High-Conductivity Thermal Gap Filling
  • Soft Compliant Interface Contact
  • Single-Side Adhesive Placement

Product Description

Laird A10095-02 - Tpli 230, A1, 8 x 8 in is a 0.75 mm boron-nitride-filled silicone thermal gap filler sheet with adhesive on one side. The soft, compliant, electrically insulating material has 6.0 W/(m K) thermal conductivity for filling interfaces between heat-generating components and heat-transfer surfaces. Typical properties include Shore 00 70 hardness, 1.4 g/cm^3 density, and a -45 to 200 deg C temperature range. The 8 x 8 in preformed sheet combines gap filling, thermal transfer, and placement backing in an exact ready-to-convert part configuration.

Key features

  • Thermal gap filling: Thermal conductivity is 6.0 W/(m K) by ASTM D5470.
  • Soft compliant sheet: The silicone gap filler has typical Shore 00 70 hardness.
  • Single-side adhesive: The A1 configuration includes adhesive on one side.

Applications

Thermal gap filling between heat-generating components and heat sinks, spreaders, housings, or other heat-transfer surfaces.

Technical Specifications

General Properties
Density (g)
1.4 g/cm3
Product Type
Boron nitride filled silicone sheet
Thermal Properties
Thermal Conductivity
6.0 W/m.K
Electrical Properties
Volume Resistivity
5x10^13 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical product-selection data for the exact A10095-02 part configuration and are not specifications.

PropertyValueUnitMethod / condition
Nominal thickness0.75mmExact A10095-02 part
Sheet size8 x 8inExact A10095-02 part
Adhesive backingOne sideA1 configuration
Thermal conductivity6.0W/(m K)ASTM D5470; typical
Density1.4g/cm^3Helium pycnometer; typical
Hardness70Shore 00ASTM D2240; typical
Temperature range-45 to 200deg CTypical
Volume resistivity5 x 10^13ohm-cmASTM D257; typical