INSULCURE 26
Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations
Main features
- Very-Large-Casting Epoxy Hardening
- Extended 120-Minute Pot-Life Window
- Low-Viscosity Material Handling
Product Description
Insulcure 26 is an epoxy curing agent for very large castings and good impact performance. Supplied viscosity is 800 cP at 25 deg C by ASTM D2393, while the 120-minute pot life provides a longer working window for casting preparation. The cure schedule is 36 hours at 25 deg C. Supplied as a single hardener product, Insulcure 26 is used with epoxy systems where extended processing time is required for large casting operations.
Key features
- Very large casting use: The curing agent is intended for very large castings.
- Extended pot life: Pot life is 120 minutes.
- Low supplied viscosity: Viscosity is 800 cP at 25 deg C by ASTM D2393.
Applications
Epoxy curing and hardening for very large castings.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Values are product-selection data for the curing agent and are not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Viscosity | 800 | cP | 25 deg C; ASTM D2393 |
| Pot life | 120 | min | Condition not stated |
| Cure schedule | 36 | h | 25 deg C |