HumiSeal UV23LV is a one-part, low-viscosity UV/cationic epoxy adhesive for electronic and industrial bonding. Typical viscosity is 2,500 cP, and the adhesive bonds metals, glass, ceramics, and plastics. UV exposure brings the adhesive to handling condition in 30 seconds, while secondary cure is completed in 24 hours at room temperature or 1 hour at 150 deg C. After cure, the clear adhesive reaches Shore D80 hardness and a typical operating-temperature range of -10 to 200 deg C. Its low-viscosity format combines fast light response with secondary cure for bonded electronic and industrial assemblies.

Key features

  • Low-viscosity dispensing: Typical supplied viscosity is 2,500 cP.
  • Fast UV handling: Handling condition is reached in 30 seconds with UV exposure.
  • Secondary cure flexibility: Full cure is 24 hours at room temperature or 1 hour at 150 deg C.

Applications

Electronic and industrial bonding of metals, glass, ceramics, and plastics.

Product Family

HUMISEAL UV23LV

Loading pricing…

Technical Specifications

General Properties
Component System
One
Thermal Properties
Operating Temperature
-10 to 200 °C
Physical Properties
Viscosity
2,500 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical product-selection data and are not specifications.

PropertyValueUnitMethod / condition
Viscosity2,500cPAs supplied; typical
Handling time30secWith UV exposure; typical
Full cure24hRoom temperature; secondary cure; typical
Accelerated full cure1h150 deg C; secondary cure; typical
Technical properties

After-processing / final-state properties

Values describe the cured material and are typical product-selection data, not specifications.

PropertyValueUnitMethod / condition
ColorClearCured material
HardnessD80Shore DCured material; typical
Operating temperature-10 to 200deg CCured material; typical range