FIXMASTER FLEX 80

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

FIXMASTER FLEX80

Main features

  • Two-Part Black Urethane
  • Casting and Rebuilding Parts
  • Corrosion, Wear, and Impact Exposure

Product Description

LOCTITE MR FLEX 80 is a two-part, thick black polyurethane compound for casting and rebuilding parts exposed to corrosion, wear, and impact. LOCTITE MR FLEX 80 is the current designation associated with the former FIXMASTER FLEX80 name. It is used for repair by casting and rebuilding parts subject to corrosion, wear, or impact exposure. Its product role is repair and casting rather than general-purpose structural bonding.

Key features

  • Two-Part Black Urethane: The material is a thick black polyurethane compound supplied as a two-part system.
  • Casting and Rebuilding Parts: The castable system is used to rebuild and repair parts.
  • Corrosion, Wear, and Impact Exposure: The castable urethane is used on parts exposed to corrosion, wear, and impact.

Applications

Casting and rebuilding parts exposed to corrosion, wear, and impact.

Technical Specifications

General Properties
Appearance
Thick black liquid
Component System
Two Part (Resin | Hardener)
Mechanical Properties
Elongation
237 %
Thermal Properties
Glass Transition Temperature (Tg)
<-50 °C
Thermal Conductivity
0.16 W/m.K
Electrical Properties
Volume Resistivity
15×10¹² Ohms⋅cm
Other Properties
Storage Temperature
8 °C to 21 °C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers