ECCOSORB SF-6.0

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ECCOSORB SF-6.0

Main features

  • 6.0 GHz Absorber Tuning
  • 163 deg C Maximum Operating Temperature
  • PSA or On-Drawing Options

Product Description

Eccosorb SF-6.0 is a black silicone free-space elastomer microwave absorber grade tuned for 6.0 GHz. It is used on flat or curved metallic surfaces for narrow-band reflectivity reduction and surface-current attenuation. Standard 12X12 NA part 21459101 has a typical density of 3.50 g/cm^3, Shore A hardness of 73, a maximum operating temperature of 163 deg C, and listed reflectivity greater than -20 dB at 6.0 GHz. That standard part measures 305 x 305 mm and 2.18 mm thick. Laird also lists PSA and on-drawing configuration options for the grade.

Key features

  • 6.0 GHz Design Frequency: The grade is tuned for free-space absorption at this frequency.
  • 163 deg C Maximum Operating Temperature: Standard part 21459101 carries this listed operating-temperature limit.
  • About 2.18 mm Standard-Part Thickness: Part 21459101 is supplied as an approximately 305 x 305 mm sheet at this thickness.

Applications

Bonding to flat or curved metallic surfaces for narrow-band microwave reflectivity reduction; radar nacelles; cavity-backed or shrouded telecommunications antennas; surface-current attenuation on metal surfaces; magnetron housings. Not specified for use inside a cavity.

Product Family

ECCOSORB SF-6.0

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Service temperature
Max 163 °C
Mechanical Properties
Elongation
20 - 100 %
General Properties
Density (g)
2.4-4.5 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

Values below apply to standard 12X12 NA part 21459101; other SF-6.0 configurations may differ.

PropertyValueUnitMethod / condition
Density3.50g/cm^3Standard 12X12 NA part 21459101; typical
Hardness73Shore AStandard 12X12 NA part 21459101; typical
Sheet dimensions305 x 305mmStandard 12X12 NA part 21459101
Thickness2.18mmStandard 12X12 NA part 21459101
Technical properties

After-processing / final-state properties

Values below apply to standard 12X12 NA part 21459101; other SF-6.0 configurations may differ.

PropertyValueUnitMethod / condition
Design frequency6.0GHzStandard 12X12 NA part 21459101; typical
Reflectivity>-20dBAt 6.0 GHz; standard 12X12 NA part 21459101; listed value
Maximum operating temperature163deg CStandard 12X12 NA part 21459101

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers