DOWSIL SE 9157
Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other
Main features
- 6-Minute Tack-Free Time
- 5,675 cP Viscosity
- 27 kV/mm Dielectric Strength
Product Description
DOWSIL SE 9157 Conformal Coating is a one-part, translucent, medium-viscosity silicone conformal coating for electronic assemblies. It cures at room temperature without added solvents and reaches a typical tack-free condition in 6 minutes at 25 deg C. A 5,675 cP viscosity supports syringe, brush, flow-coating, and spray application. After cure, the soft elastomer has a typical elongation of 180% and dielectric strength of 27 kV/mm. Applications include rigid and flexible circuit boards, connectors, sensors, and spot protection on components. Mild heat up to 60 deg C can accelerate cure for in-line processing.
Key features
- 6-Minute Tack-Free Time: This surface-dry milestone is distinct from full cure.
- 5675 cP Coating Viscosity: Typical as-supplied viscosity characterizes the medium-viscosity coating.
- 180% Cured Elongation: Typical cured tensile strength is 90 psi.
Applications
Rigid and flexible circuit boards; connectors; sensors; spot protection on components.
TDS, SDS & Technical Documents
Technical Specifications
Physical Properties
General Properties
Mechanical Properties
Electrical Properties
Additional Information
As-supplied properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Viscosity | 5,675 | cP | Typical |
| Nonvolatile content | 96.9 | % | Typical |
| Shelf life | 360 | days | At 25 deg C; typical |
Cured coating properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Specific gravity | 0.995 | - | Cured; typical |
| Tensile strength | 0.6 | MPa | Typical |
| Elongation | 180 | % | Typical |
| Dielectric strength | 27 | kV/mm | JIS K 6249; typical |
| Volume resistivity | 4.0E15 | ohm*cm | JIS K 6249; typical |