DOWSIL 7094

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DOWSIL 7094

Main features

  • Self-Leveling Flowable Placement
  • 400% Cured Elongation
  • 25-Minute Skin-Over Time

Product Description

DOWSIL 7094 Flowable Sealant flows and self-levels into gaps where a one-part, neutral-cure silicone sealant is required for sealing or bonding. The black or white viscous liquid has a typical density of 1.30 g/cm^3 and viscosity of 28,000 mPa s, allowing flow into gaps and airless-spray application. At 23 deg C and 50% relative humidity, it skins in about 25 minutes, becomes tack-free in about 50 minutes and cures inward from the exposed surface. After seven days under those conditions, the sealant has Shore A 19 hardness, 400% elongation and 1.2 MPa tensile strength.

Key features

  • Flowable self-leveling rheology: Typical viscosity is 28,000 mPa s for gap filling and spray application.
  • 25-minute skin-over time: Supports tooling and assembly before surface cure.
  • Flexible cured seal: Typical elongation is 400% with Shore A 19 hardness.

Applications

Sealing and bonding applications requiring a low-viscosity, self-leveling silicone sealant.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black or white, viscous liquid
Density (g)
1.30 g/cm3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
28,000 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
400 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and cure-development properties. Values are not specifications.

Property Value Unit Method / condition
Appearance Black or white viscous liquid As supplied
Density 1.30 g/cm^3 CTM0097B
Viscosity 28000 mPa s CTM0050
Skin-over time 25 min CTM0098; 23 deg C and 50% RH
Tack-free time 50 min CTM0095A; 23 deg C and 50% RH
Cure depth About 2 mm After 24 hr at room temperature and 50% RH
Shelf life 12 months Below 30 deg C in original unopened container
Technical properties

After-processing / final-state properties

Typical mechanical properties after seven days in air at 23 deg C and 50% relative humidity.

Property Value Unit Method / condition
Tensile strength 1.2 MPa CTM0137A
Elongation at break 400 % CTM0137A
Modulus at 100% 0.36 MPa CTM0137A
Hardness 19 Shore A CTM0099