DOWSIL 3-8209

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

DOWSIL 3-8209

Main features

  • 1:1 Silicone Foam Mixing
  • 45 Shore 00 Cured Hardness
  • Integrated Compression Gasket Formation

Product Description

DOWSIL 3-8209 Silicone Foam is a two-part, gray silicone foam system dispensed and cured directly on parts to form an integrated compression gasket. Parts A and B mix 1:1 and cure at room temperature. Typical cured hardness is 45 Shore 00. The foam retains low compression set at high service temperatures and remains stable and flexible across a wide temperature range. Applications include automotive parts, electrical-device housings, exterior lighting, and domestic appliance components.

Key features

  • Equal-ratio foam mixing: Parts A and B use a 1:1 mix ratio before dispensing.
  • Cured foam hardness: Typical cured hardness is 45 Shore 00.
  • Integrated compression gasket formation: The foam is dispensed and cured directly on parts to form a compression gasket.

Applications

Integrated compression gasketing for automotive parts, electrical-device housings, exterior lighting, and domestic appliance components.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two Part (A/B)
Physical Properties
Tack-Free Time
maximum 10 minutes

Leading Brands Trust in Our Products and Services