BOSTIK LADH1231
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- Fast-Drying Spray Application
- Green Strength with Creep Resistance
- Pressure and Vacuum Forming
Product Description
Bostik LADH1231 is a one-component solvent-based liquid adhesive for automotive interior-trim assembly. The medium-viscosity tan adhesive is sprayable and designed for pressure bonding and vacuum forming. It bonds fabric, nonwoven materials, and polyolefin foam to fiberboard, ABS, and unprimed polypropylene within automotive interior-trim applications. The formulation combines fast dry time with green strength and creep resistance for formed and pressure-bonded interior components that must be handled through the assembly process.
Key features
- Fast spray processing: Sprayable liquid with fast dry time for automotive interior-trim assembly.
- Green strength and creep resistance: Formulation combines green strength with creep resistance for interior-trim bonding.
- Pressure and vacuum forming: Designed for pressure-bonding and vacuum-forming applications.
Applications
Pressure- and vacuum-forming of fabric, nonwoven materials, and polyolefin foam to fiberboard, ABS, and unprimed polypropylene in automotive interiors.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Physical Properties
Additional Information
As-supplied properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Tan/brown | Typical physical property | |
| Base polymer | Modified chloroprene | Typical physical property | |
| Flash point | -18 | deg F | Closed cup; typical |
| Density | 0.80 | g/cm^3 | Typical physical property |
| Nonvolatile content | 19 | % | Typical physical property |
| Viscosity | 200 | cP | Brookfield RVT #2/20; 25 deg C; typical |