BOSTIK F10-634
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- Excellent Texture Retention
- Flexible Heat- and Solvent-Resistant Cure
- Controlled Aircraft Laminate Processing
Product Description
Bostik F10-634 provides a flame-retardant thermoset film adhesive for decorative laminate constructions used in aircraft interiors. The white film is supplied at a nominal 3 mil thickness and 130 g/m^2 dry-film weight. It is formulated for excellent texture retention in embossed decorative structures and shows adhesion to fluorinated films. Recommended processing is approximately 300 to 330 deg F with at least 10 minutes of heat under pressure. After cure, the adhesive remains flexible and provides heat and solvent resistance for decorative laminate constructions that require controlled texture and thermoset performance.
Key features
- Excellent texture retention: Maintains embossed decorative texture through the laminate bonding process.
- Controlled heat bonding: Recommended processing is about 300 to 330 deg F with at least 10 minutes of heat under pressure.
- Flexible resistant cure: The cured film remains flexible and provides heat and solvent resistance.
Applications
Bonding decorative laminate constructions used in aircraft interiors.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | White film | As supplied | |
| Dry film weight | 130 | g/m^2 | TDS also gives 0.027 lb/ft^2 |
| Dry film thickness | 3.0 | mil | Nominal |
| Volatiles | <3.0 | % | As supplied |
| Shelf life | 1 | year | Recommended storage conditions |
| Storage temperature | 40 to 80 | deg F | Dry storage; TDS also gives 4 to 27 deg C |