BONDERITE S-ST 6930
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other
Main features
- Hydrogen-Peroxide-Activated Paint Removal
- Vertical and Overhead Surface Cling
- High-Pressure Water-Rinse Removal
Product Description
BONDERITE S-ST 6930 AERO is a low-odor, thixotropic aerospace paint stripper activated with hydrogen peroxide for removal of epoxy, epoxy-primer, polyurethane, and related catalyzed coating systems. It is intended for controlled paint removal on approved aluminum, mild steel, high-strength steel, cadmium-plated steel, and titanium substrates, while magnesium is outside the documented scope. The material is applied by non-atomizing spray and provides cling on vertical and overhead surfaces. Following stripping, loosened coating can be removed by squeegee and high-pressure water rinse, supporting a defined removal sequence for aerospace maintenance operations.
Key features
- Hydrogen-Peroxide Activation: Uses a hydrogen-peroxide-activated stripping system for catalyzed aerospace coatings.
- Vertical and Overhead Cling: The thixotropic material maintains contact on vertical and overhead surfaces.
- Defined Rinse-Off Process: Loosened coating is removed by squeegee followed by high-pressure water rinse.
Applications
Aerospace paint removal from approved aluminum, mild steel, high-strength steel, cadmium-plated steel, and titanium substrates using the specified activated stripping process.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| VOC | 647 | g/L | As supplied |
| VOC vapor pressure | Less than 2 | mm Hg | TDS value |
| Storage temperature | 2 to 40 | deg C | Recommended storage range |