BONDERITE M-ZN 181 X

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

BONDERITE M-ZN 181

Main features

  • Lubricant-Retaining Phosphate Layer
  • Reduced Metal-on-Metal Friction
  • Batch-to-Extrusion Process Coverage

Product Description

BONDERITE M-ZN 181 X is a zinc-phosphate conversion-coating series for steel before cold-forming and drawing operations. It forms a nonmetallic phosphate layer that retains lubricant and reduces metal-on-metal friction during forming. The series is supplied as separate Make-Up and Replenisher grades rather than as a kit. Process configurations cover batch, strand, tubing, and extrusion operations, with bath preparation and control values assigned by process. Applications include wire drawing and other steel cold-forming operations where lubricant retention and smoother surface formation are important.

Key features

  • Cold-forming phosphate layer: Retains lubricant on steel during forming and drawing.
  • Separate MU and R grades: Make-Up and Replenisher are supplied as distinct process grades.
  • Process-specific bath control: Supports batch, strand, tubing, and extrusion configurations.

Applications

Applications include zinc-phosphate treatment of steel before batch, strand, tubing, extrusion, wire-drawing, and other cold-forming operations.

Product Family

BONDERITE M-ZN 181 X

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Bath-preparation values apply to BONDERITE M-ZN 181 X Make-Up (MU); Replenisher data are not included.

PropertyValueUnitMethod / condition
Initial bath charge - batch87lbMU; 7 gal per 100 gal bath
Initial bath charge - strand304lbMU; 24.5 gal per 100 gal bath
Initial bath charge - tubing109lbMU; 8.8 gal per 100 gal bath
Initial bath charge - extrusion174lbMU; 14 gal per 100 gal bath
 