BONDERITE M-AD 500

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

BONDERITE M-AD 500

Main features

  • Dual Zinc and Iron Bath Adjustment
  • Controlled 1:4 Pre-Dilution
  • Stepwise pH Correction

Product Description

BONDERITE M-AD 500 is an alkaline liquid additive for pH and free-acid adjustment in metal-pretreatment baths. It reduces free acid in zinc-phosphating baths and increases pH in iron-phosphating processes. For a 0.1-point free-acid reduction in 1,000 L of bath, the guidance specifies 0.5 kg, equivalent to 0.44 L, added slowly after approximately 1:4 pre-dilution. Small-step addition, good bath agitation, and pH checks provide a controlled adjustment sequence for immersion and spray pretreatment operations.

Key features

  • Dual Bath Adjustment: Reduces free acid in zinc-phosphating baths and raises pH in iron-phosphating processes.
  • Controlled Pre-Dilution: Use approximately 1:4 pre-dilution before slow addition to an agitated bath.
  • Stepwise pH Control: Add in small steps, mix thoroughly, and measure pH between additions.

Applications

Free-acid and pH adjustment in zinc- or iron-phosphating baths using immersion or spray processing.

Product Family

BONDERITE M-AD 500

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear liquid
Chemistry Type
Alkaline solution
Density (g)
1.1 g/cm3
Product Type
Material category or functional product class.
Additive for pretreatment baths (pH-adjustment)

Additional Information

Technical properties

As-supplied properties

PropertyValueUnitMethod / condition
AppearanceClear liquid-As supplied
Chemical characterAlkaline solution-As supplied
DensityApproximately 1.1g/cm^3As supplied
Storage temperature5 to 40deg CUnopened original packaging
Shelf life30monthsUnopened original packaging