BONDERITE C-AK 6751-L

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

BONDERITE C-AK 6751-L

Main features

  • Multi-Soil Metal Cleaning
  • Room-Temperature Water Rinsing
  • 30 to 60 deg C Operation

Product Description

BONDERITE C-AK 6751-L AERO is a brown liquid alkaline cleaning agent for ferrous and nonferrous metal surfaces. It removes shop soils, lubricating oils, light drawing oils, and waxes, then rinses from metal with room-temperature water. The cleaner functions from 30 to 60 deg C, giving a defined temperature window for controlled cleaning operations. Its liquid form and water-rinsable behavior fit parts-cleaning processes that require removal of common manufacturing soils from metal surfaces. Also known as Turco 6751-L, the exact AERO grade is supplied as a specialty cleaner.

Key features

  • Multi-soil metal cleaning: Removes shop soils, lubricating oils, light drawing oils, and waxes from ferrous and nonferrous metals.
  • Room-temperature water rinsing: Rinses from metal surfaces with room-temperature water after cleaning.
  • Defined operating range: Functions from 30 to 60 deg C for controlled cleaning operations.

Applications

Cleaning ferrous and nonferrous metal surfaces to remove shop soils, lubricating oils, light drawing oils, and waxes.

Product Family

BONDERITE C-AK 6751-L

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Operating Temperature
30 to 60 °C