ARALDITE 2023-30

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

ARALDITE 2023-30

Main features

  • Room-Temperature Methacrylate Cure
  • Up to 30 mm Gap Fill
  • 15.5 MPa Lap Shear

Product Description

ARALDITE 2023-30 A/B is a two-component, room-temperature-curing flexible methacrylate structural adhesive supplied as a thixotropic paste. The adhesive can fill gaps up to 30 mm and has an as-supplied density of 1.09 g/cm^3. Cured performance includes 15.5 MPa lap shear strength under ISO 4587 at 23 deg C on sandblasted aluminum 5754, 22 MPa tensile strength under ISO 527 at 23 deg C, and 62 Shore D hardness under ISO 868 at 23 deg C. Applications include composite bonding in the manufacture of large structures.

Key features

  • Room-temperature cure: Two-component methacrylate system cures at room temperature.
  • Up to 30 mm gap filling: The thixotropic paste can fill gaps up to 30 mm.
  • 15.5 MPa lap shear: ISO 4587 at 23 deg C on sandblasted aluminum 5754.

Applications

Composite bonding in the manufacture of large structures.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Bright grey
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (F 323-30 MIN | Hardener F 323)
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
35 - 50 minutes
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.09
Physical Properties
Open time
> 30 minutes

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Physical formPasteThixotropic, as supplied
Density1.09g/cm^3As supplied
Maximum gap filling30mmUp to; thixotropic paste
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Hardness62Shore DISO 868 at 23 deg C
Tensile strength22MPaISO 527 at 23 deg C
Cured density1.29g/cm^3ISO 1183 at 23 deg C, cured
Glass transition temperature40.8deg CISO 6721 onset
Lap shear strength15.5MPaISO 4587 at 23 deg C, sandblasted aluminum 5754