ABLESTIK 539IA
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- Polyester-Carrier Epoxy Film
- 1-Month Work Life at 25 deg C
- 1-Hour 150 deg C Cure
Product Description
LOCTITE ABLESTIK 539IA is a transparent, non-conductive heat-cure epoxy film adhesive for LCD assembly and bonding difficult metals, plastics, and ceramics. Its polyester carrier provides a uniform bond-line construction, with the film remaining non-conductive after cure. Work life is 1 month at 25 deg C, and heat-cure options are 1 hour at 150 deg C or 2 hours at 125 deg C. Shelf life is 365 days at 0 deg C.
Key features
- Polyester-carrier construction: Transparent epoxy film uses a polyester carrier with a uniform bond-line format.
- One-month work life: Work life is 1 month at 25 deg C.
- Dual heat-cure schedules: Heat cure is 1 hour at 150 deg C or 2 hours at 125 deg C.
Applications
LCD assembly and bonding difficult metals, plastics, and ceramics.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Additional Information
As supplied
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Transparent film | As supplied | |
| Carrier | Polyester | As supplied | |
| Work life | 1 | month | 25 deg C |
| Shelf life | 365 | days | 0 deg C |