3M 48

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

3M 48

Main features

  • 3 mil Unfused PTFE Tape
  • Typical -268 to 260 deg C Stability
  • Five-Year Shelf Life Under Stated Storage

Product Description

Scotch 48 Thread Sealant and Lubricant is an unfused PTFE fluorocarbon film tape for sealing and lubricating threaded connections. The milky-white, conformable film wraps directly around the threads without liquid dispensing or curing. Typical film thickness is 3 mil, tensile strength is 5.9 lb/in, and elongation at break is 26%. Typical temperature stability extends from -268 to 260 deg C; ventilation is required above 204 deg C because the film can release toxic fumes. Shelf life is five years from manufacture when kept in a clean, dry location at 70 deg F and 40 to 50% relative humidity.

Key features

  • 3 mil unfused PTFE film: The conformable dry tape provides both the sealing and lubrication layer around threads.
  • Typical -268 to 260 deg C film stability: Use above 204 deg C requires ventilation because PTFE film can release toxic fumes.
  • Five-year storage life: Shelf life runs from manufacture at 70 deg F and 40 to 50% relative humidity in clean, dry storage.

Applications

Thread sealing and lubrication, including high-pressure oxygen-line use within the manufacturer's documented conditions.

Technical Specifications

Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
26 %

Additional Information

Technical properties

As-supplied / before-processing properties

Values reflect legacy 2000 product data and are not current specifications.

PropertyValueUnitMethod / condition
MaterialUnfused PTFE fluorocarbon film-Thread-seal tape
Tape thickness3milTypical legacy product data
Application formDry tape-Applied directly to threaded connections
Shelf life5yearsUnder stated storage conditions

Leading Brands Trust in Our Products and Services